Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930197
EISBN: 978-1-62708-359-1
... or by integranular separation. However, all of the other data are necessary to ensure that a more obscure cause of failure is not missed. The outcome of the failure analysis should usually be a recommendation that will avoid recurrence. Such recommendations generally consist of an eliminate-the-cause procedure...