Published: 01 January 2017
Fig. 6.4 Effects of average plant water purity shown in field correlations of the core-component cracking behavior for (a) stainless steel IRM/SRM instrumentation dry tubes, and (b) creviced stainless steel safe ends (C) creviced Inconel 600 shroud-head bolts, also showing the predicted More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000133
EISBN: 978-1-62708-313-3
... 830 120 705 102 620 90 605 88 28 22 20 Inconel 597 Bar 1220 177 1140 165 930 135 760 110 720 104 665 96 15 15 16 Inconel 600 Bar 660 96 560 81 260 38 285 41 220 32 180 26 45 41 70 Inconel 601 Sheet 740 107 725 105 290 42 455 66 350 51 220...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200295
EISBN: 978-1-62708-354-6
... low carbon content. CW6MC - Similar to Inconel 625 in composition. CY40 - Similar to Inconel 600. Heat Treatment Proper heat treatment of the nickel-base alloys is critical. Except for some rare applications, these alloys are solution treated to improve their corrosion properties...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000117
EISBN: 978-1-62708-313-3
... … … Inconel 102 (a) 7 … 67 0.5 0.5 15 2.9 3 2.9 … 0.005 0.06 0.03 … … … … … 0.02 … … Inconel 120 (a) … 14 bal. 0.25 2.5 21 4 … 2 … 0.005 0.04 … … … … 0.05 … … … … Inconel 600 (b) 8 … 76 … … 15.5 … … … … … 0.08 … … … … … … … 0.25...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090135
EISBN: 978-1-62708-266-2
... in the presence of small concentrations of oxidizing impurities. The Ni-Fe-Cr alloys, such as alloys 600 (UNS N06600) and 800 (N08800), are used widely in the power generation industry as steam generator tubing. The Ni-Fe-Cr-Mo alloys, such as alloy 825 (N08825) and alloy 2550 (N06255), are used in a variety...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030074
EISBN: 978-1-62708-282-2
... turbines, heat treatment equipment N06230 Haynes 230 22.0 55.0 5.0 max 2.0 … … 0.35 3.0 max 0.10 14.0 W, 0.015 max B, 0.02 La Gas turbines, superheater tubes N06600 Inconel 600 15.5 76.0 … … … … … 8.0 0.08 0.25 Cu Furnace components N06601 Inconel 601 23.0 60.5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280011
EISBN: 978-1-62708-267-9
... 620 90 605 88 28 22 20 Inconel 597 Bar 1220 177 1140 165 930 135 760 110 720 104 665 96 15 15 16 Inconel 600 Bar 660 96 560 81 260 38 285 41 220 32 180 26 45 41 70 Inconel 601 Sheet 740 107 725 105 290 42 455 66 350 51 220 32 40 34 78...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000001
EISBN: 978-1-62708-313-3
... concerns when selecting the material. An additional consideration in combustor design is the complicated shape, which requires a number of sheet metal forming operations and joining methods. Superalloys such as Nimonic 75, Hastelloy X, Inconel 600, and Haynes 188 are commonly selected for this application...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280001
EISBN: 978-1-62708-267-9
... 14.0 … … 0.35 3.0 max 0.10 0.015 max B, 0.02 La   Inconel 600 15.5 76.0 … … … … … … 8.0 0.08 0.25 Cu   Inconel 601 23.0 60.5 … … … … … 1.35 14.1 0.05 0.5 Cu   Inconel 617 22.0 55.0 12.5 9.0 … … … 1.0 … 0.07 …   Inconel 625 21.5 61.0 … 9.0 … 3.6...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430087
EISBN: 978-1-62708-253-2
... to these alloys by precipitation hardening. Inconel 617, Inconel 671, Inconel 740, Inconel 718, and HR6W, listed in Table 4.5 , are typical examples of nickel-base superalloys used for SC and USC boiler applications. Haynes 230, Inconel 740, and CCA 617 are selected for heavy sections, high-temperature...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280135
EISBN: 978-1-62708-267-9
... Inconel 600 900 1650 1 1010 1850 ¼ (d) Inconel 601 … … … 980 1800 … Inconel 625 870 1600 1 980 1800 1 Inconel 690 … … … 1040 1900 ½ Inconel 718 (c) (c) … 955 1750 1 Inconel X-750 880 (e) 1625 (e) … 1035 1900 ½ Nimonic 80A (c) (c) … 1080...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000009
EISBN: 978-1-62708-313-3
... carbide precipitation, such as 19-9DL (18-8 stainless steel with slight chromium and nickel adjustments, additional solution hardeners, and higher carbon) and Inconel-800H (21% Cr and high nickel with small additions of titanium and aluminum, which produce some γ′ phase) ( Ref 1 ). The field of stainless...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170290
EISBN: 978-1-62708-297-6
... … … … … 0.75 0.58 44.8 0.35 … Nickel-base Haynes 214 N07214 16.0 76.5 … … … … … 4.5 3.0 0.03 Haynes 230 N06230 22.0 55.0 5.0 max 2.0 14.0 … … 0.35 3.0 max 0.10 0.015 max B, 0.02 La Inconel 600 N06600 15.5 76.0 … … … … … … 8.0 0.08 0.25 Cu Inconel 601...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850562
EISBN: 978-1-62708-260-0
...., °C Time, min <30 1 1-2 2-4 2-4 25 s 5-10 s <25 <35 4-6 70 Comments Allow solution to age for 24 h before use. Use Fe or Al cathode (Jacquet and Rocquet). For Ni 200 and Ni 270 For Monel 400. For Inconel 625. For Incoloy 800, not good for Inconel 718 orInconel 600 (Evans and Lloyd). Used for Monel 400...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170495
EISBN: 978-1-62708-297-6
... Nicrofer 6629 (B-4) N10629 bal 0.5–1.5 1.0–6.0 2.5 26.0–30.0 … … … 0.1–0.5 0.01 1.5 0.05 … … Nickel-chromium-iron alloys Inconel 600 N06600 72.0 min (b) 14.0–17.0 6.0–10.0 … … … … … … 0.15 1.0 0.5 … 0.5 Cu Inconel 601 N06601 58.0–63.0 21.0–25.0 bal...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030019
EISBN: 978-1-62708-282-2
... lead-tin solder Type 304 stainless steel (active) Type 316 stainless steel (active) Lead Tin Copper alloy C28000 (Muntz metal, 60% Cu) Copper alloy C67500 (manganese bronze A) Copper alloys C46400, C46500, C46600, C46700 (naval brass) Nickel 200 (active) Inconel alloy 600...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080445
EISBN: 978-1-62708-304-1
... … … … Bal … … … … Cu: 55.0 CUPRO 107 … … … Bal … 0.8 … … Cu: 68.0, Mn: 1.1 INCONEL 600 N06600 0.08 (a) 15.5 Bal … 8.0 … … … INCONEL 601 N06601 0.10 (a) 23.0 Bal … 14.4 … … Al: 1.4 Nicrofer 6025HT (602CA) N06025 0.2 25 Bal … 10 … … Al: 2.1, Ti: 0.15, Y...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930329
EISBN: 978-1-62708-359-1
... … Hastelloy X 8.21 1260–1355 2300–2470 15.1 (b) 9.1 1180 Hastelloy S 8.76 1335–1380 2435–2515 13.3 (b) … … Inconel 600 8.41 1355–1415 2470–2575 15.1 (b) 14.8 1030 Inconel 601 8.05 1300–1370 2375–2495 15.3 (b) 11.3 1190 Inconel 617 8.36 1330–1375 2430–2510 13.9 (b...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280203
EISBN: 978-1-62708-267-9
... and Inconel 600 solution-hardened nickel-base superalloys, and Inconel X-750, a lower-strength nickel-base precipitation-hardening superalloy. The sequence of operations performed on these stampings was either to form, degrease, remove metal contamination, anneal, and descale, or to immerse in molten salt...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280189
EISBN: 978-1-62708-267-9
..., Hastelloy S, Hastelloy X, Inconel 600, Inconel 601, Refractoloy 26, Udimet 630 Ni Wrt 5 TD-nickel Ni Cast 1 Hastelloy B, Hastelloy C, ASTM A297, grades HW and HX, ASTM A608 grades HW50, HX50 Ni Cast 2 B-1900, IN-100 (Rene 100), IN-738, IN-792, Inconel 713C, Inconel 718, M252, MAR-M-200, MAR-M...