...) 1 (c) … … .35 (c) Hastelloy C-276 (b) 5 … 59 … … 15.5 16 3.7 … … … 0.02 (c) … … … … … … … … … Hastelloy C-4 (b) 19.5 2 (c) bal. … 0.7 (c) 16 16 2(Nb+Ta) … .015 (c) … … … … 0.08 (c) 1 (c) … 2 … Hastelloy G (b) 19.5 2.5 (c) bal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030074
EISBN: 978-1-62708-282-2
... Hastelloy B-3 68.5 1.5 … 28.5 1.5 … … Nickel-chromium-molybdenum alloys N10276 Hastelloy C-276 59 16 … 16 5 4 … N06455 Hastelloy C-4 68 16 … 16 … … … N06022 Hastelloy C-22 59 22 … 13 3 3 … N06200 Hastelloy C-2000 59 23 1.6 16 … … … N06059...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170495
EISBN: 978-1-62708-297-6
... V Hastelloy C-4 N06455 bal 14.0–18.0 3.0 2.0 14.0–17.0 … … 0.70 … 0.015 1.0 0.08 … … Hastelloy C-22 N06022 bal 20.0–22.5 2.0–6.0 2.5 12.5–14.5 2.5–3.5 … … … 0.015 0.5 0.08 … 0.35 V Hastelloy C-276 N10276 bal 14.5–16.50 4.0–7.0 2.5 15.0–17.0 3.0–4.5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030112
EISBN: 978-1-62708-282-2
... to boiling 60% H 2 SO 4 + 8% HCl Fig. 9 Effect of 1 h aging treatment on corrosion resistance of three Hastelloy alloys in 50% H 2 SO 4 + 42 g/L Fe 2 (SO 4 ) 3 . Source: Ref 10 Fig. 10 Typical microstructure of the HAZ of a multipass submerged arc weld in Hastelloy alloy C-276. Source...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280001
EISBN: 978-1-62708-267-9
... 9.0 0.6 … … 2.0 15.8 0.15 …   Hastelloy C-276 15.5 59.0 … 16.0 3.7 … … … 5.0 0.02 max …   Haynes HR-120 25.0 37.0 3.0 2.5 2.5 0.7 … 0.1 33.0 0.05 0.7 Mn, 0.6 Si, 0.2 N, 0.004 B   Haynes HR-160 28.0 37.0 29.0 … … … … … 2.0 0.05 2.75 Si, 0.5 Mn...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080445
EISBN: 978-1-62708-304-1
... 2.5 6.0 24.0 … … HASTELLOY S N06635 0.02 (a) 15.5 Bal … 3.0 (a) 14.5 … La: 0.05, B: 0.015 (a) HASTELLOY N N10003 0.06 7.0 Bal … 5.0 (a) 16.5 … … HASTELLOY C-22 N06022 0.01 (a) 22.0 Bal 2.5 (a) 3.0 13.0 3.0 … HASTELLOY C-276 N10276 0.01 (a) 15.5 Bal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820203
EISBN: 978-1-62708-339-3
... (1000 °F) Nitric acid (A 262-C) 240 0.025 (1) N10276 Hastelloy C-276 None Ferric sulfate (G 28-A) 24 1 (40) N06455 Hastelloy C-4 None Ferric sulfate (G 28-A) 24 0.43 (17) N06110 Allcorr None Ferric sulfate (G 28-B) 24 0.64 (25) N10001 Hastelloy B None 20% hydrochloric...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910193
EISBN: 978-1-62708-250-1
... Effects Corrosion is an activation-controlled chemical reaction, the rate of which is greatly affected by temperature. Typically, corrosion rate increases significantly as temperature increases. A rule of thumb is that the corrosion rate will double for each 10 °C (18 °F) increase in temperature...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170290
EISBN: 978-1-62708-297-6
... 1.5 max 9.0 0.6 … … 2.0 15.8 0.15 … Hastelloy C-276 N10276 15.5 59.0 … 16.0 3.7 … … … 5.0 0.02 max … Haynes HR-120 N08120 25.0 37.0 3.0 2.5 2.5 0.7 … 0.1 33.0 0.05 0.7 Mn, 0.6 Si, 0.2 N, 0.004 B Haynes HR-160 N12160 28.0 37.0 29.0 … … … … … 2.0 0.05...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280189
EISBN: 978-1-62708-267-9
..., Inconel 700, Nimonic 90, Nimonic 95, Rene 41, Rene 63, Udimet 500, Udimet 700, Udimet 710 Ni Wrt 3 Rene 95, Rene 77, Inconel MA 6000 (b) Ni Wrt 4 Hastelloy B, Hastelloy B-2, Hastelloy C, Hastelloy C-276, Hastelloy S, Hastelloy X, Inconel 600, Inconel 601, Refractoloy 26, Udimet 630 Ni Wrt 5...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240547
EISBN: 978-1-62708-251-8
... 295 43 44 138 HB Alloy 690 Ni-29Cr-9Fe 725 105 348 50 41 88 HRB Alloy 751 Ni-15Cr-7Fe-1Nb-2Ti 1310 190 976 142 22 352 HB Nickel-chromium-molybdenum alloys Alloy C-276 Ni-15.5Cr-16Mo-5.5Fe-3.75W-1.25Co + V 785 114 372 54 62 209 HB Alloy 625 Ni-21.5Cr-9Mo-3.65Nb...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820125
EISBN: 978-1-62708-339-3
... (a) 0.01 (a) ... 0.7 (a) ... C-22 N06022 Wrought 56 0.5 (a) 13 22 3 3 0.5 (a) 0.08 (a) 0.01 (a) ... ... V 0.35 (a) C-22HS ... Wrought (age hardenable) 61 0.5 (a) 17 21 2 (a) 1 (a) 0.8 (a) 0.08 (a) 0.01 (a) 0.5 (a) ... ... C-276 N10276 Wrought 57 0.5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910331
EISBN: 978-1-62708-250-1
... time for alloy sorting is very fast, in seconds. Examples of alloy sorting are as follows: Type 304 (UNS S30400) stainless steel or type 316 (UNS S31600) Alloy C-276 (UNS N10276) or alloy 825 (UNS N08825) Carbon steel or low-alloy types These analyzers cannot measure carbon...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030096
EISBN: 978-1-62708-282-2
... 3.5 … Incoloy alloy 135 27 31 3.5 … Hastelloy alloy G 22 38 3.7 … P 12 21 61 8.6 … Inconel alloy 112 21 61 8.7 … Hastelloy alloy C-276 15 58 15.4 … Welding conditions and corrosion resistance of heat-tinted UNS S31726 stainless steel plate Table 2 Welding...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030019
EISBN: 978-1-62708-282-2
.... The combination of a passive surface with the inherent corrosion resistance of nickel-chromium alloys, such as Inconel alloy 600 and Hastelloy alloy C-276, places them in more noble positions in the traditional galvanic series. In chloride-bearing solutions, Inconel alloy 600 is reported to occupy two positions...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090135
EISBN: 978-1-62708-266-2
.... , and Scanlon J.C. , Electron Microscopic Analysis of Heterogeneous Precipitates in Hastelloy Alloy C-276 , Metall. Trans. A , Vol 13 , 1982 , p 979 10.1007/BF02643394 5.12 Brooks C.R. , Spruiell J.E. , and Stansbury E.E. , Physical Metallurgy of Nickel-Molybdenum Alloys , Int...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080147
EISBN: 978-1-62708-304-1
... (1.60) S 0.053 (2.08) 0.063 (2.48) X 0.020 (0.80) 0.071 (2.80) C-276 0.079 (3.12) 0.079 (3.12) 6B 0.014 (0.56) 0.098 (3.84) 188 0.014 (0.56) 0.116 (4.56) (a) Metal loss + average internal penetration. Source: Ref 35 Corrosion of various alloys in Ar...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820077
EISBN: 978-1-62708-339-3
... 430 430 Annealed 308(L), 309(L), 310(ELC) Annealed or as-welded 439 430, 430Ti Annealed or as-welded 442 442 Annealed 308(L), 309(L), 310(ELC) As-welded 446 446 Annealed 308(L), 309(L), 310(ELC) As-welded E-Brite 26–1 ER26–1 As-welded Inconel 112, Hastelloy C-276...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000059
EISBN: 978-1-62708-313-3
..., with such commercial examples as Hastelloy B-2 (28 weight percent Mo), Hastelloy C-276 (16 weight percent Mo), Hastelloy C-22 (13 weight percent Mo), Inconel 625 (9 weight percent Mo), and Hastelloy G-30 (5 weight percent Mo and 2.5 weight percent W) ( Ref 20 ). However, molybdenum, tungsten, and vanadium also have...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910099
EISBN: 978-1-62708-250-1
... are more susceptible to pitting than many other metals. High-alloy stainless steels containing chromium, nickel, and molybdenum are also more resistant to pitting but are not immune under all service conditions. Pitting failures of corrosion-resistant alloys, such as Hastelloy C, Hastelloy G...