Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200298
EISBN: 978-1-62708-354-6
... to thermal cycling. Standard Designations and Compositions of Cast Heat-Resistant Steel Table 22-3 Standard Designations and Compositions of Cast Heat-Resistant Steel Alloy grade ASTM specs Composition, Wt% C Mn Si P S Cr Ni Mo Nb HA 1,2,3 0.20 0.65 (a) 1.0 0.04 0.04 8...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240371
EISBN: 978-1-62708-251-8
... in ASTM A 128, with the compositions given in Table 20.15 . Composition ranges of austenitic manganese steel casting alloys Table 20.15 Composition ranges of austenitic manganese steel casting alloys ASTM A 128 grade Composition, % C Mn Cr Mo Ni Si (max) P (max) A 1.05–1.35...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310147
EISBN: 978-1-62708-286-0
.... Compositions of cast stainless corrosion resisting alloys Table 1 Compositions of cast stainless corrosion resisting alloys ACI designation Nearest AISI grade UNS Composition (a) , wt%—maximum or range %C %Mn %Si %Cr %Ni %Mo %Other Chromium alloys CA-15 410 J91150 0.15 1.00...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200404
EISBN: 978-1-62708-354-6
...</xref></bold>) Table 27-10 Composition and Heat Treatment of the Cast and Wrought Steels for Which Electrical Resistivity and Thermal Conductivity Data Are Shown in Figures 27-8 and 27-19 ( 15 ) Analysis code Composition, % Heat treatment C Si Mn S P Ni Cr Mo E10A 0.11 0.4 0.35 0.028...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060291
EISBN: 978-1-62708-261-7
... 2.4 1.1 0.40 0.40 Nb 1200 Source: Ref 12.2 Typical compositions of corrosion-resistant austenitic stainless steels Table 12.5 Typical compositions of corrosion-resistant austenitic stainless steels Alloy Designation C N Cr Ni Mo Mn Si Other Other 316L S31603...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490383
EISBN: 978-1-62708-340-9
... (1150 °F) or higher SP, VHP, HP, VHP-HP, IP rotor Cr-Mo-V steel (forging) 12%Cr steel (forging) Austenitic superalloy or equivalent (forging) Inner cylinder Cr-Mo steel (casting) 9%Cr steel (casting) 316 austenitic steel (casting or forging) Blade Heat-resisting superalloy, if needed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310123
EISBN: 978-1-62708-286-0
... of the various possible alloying elements on the key properties of martensitic stainless steels. Influence of alloying elements on ferrite, Ms, and austenite start Table 2 Influence of alloying elements on ferrite, Ms, and austenite start Element N C Ni Co Cu Mn Si Mo Cr V Al Lowering...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430027
EISBN: 978-1-62708-253-2
... be classified in a number of ways depending on the basis of classification. A brief list of some of the criteria used for classification of steels ( Ref 3.7 ) includes: Composition—plain carbon, low-alloy, and high-alloy steels Principle alloying element present—Ni steel, Cr steel, Cr-Ni steel, or Cr...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310233
EISBN: 978-1-62708-326-3
... wrought stainless steels Type UNS designation Composition (a) , % C Mn Si Cr Ni P S Other Austenitic types 201 S20100 0.15 5.5–7.5 1.00 16.0–18.0 3.5–5.5 0.06 0.03 0.25 N 202 S20200 0.15 7.5–10.0 1.00 17.0–19.0 4.0–6.0 0.06 0.03 0.25 N 205 S20500 0.12...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.sch6.9781627083546
EISBN: 978-1-62708-354-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820077
EISBN: 978-1-62708-339-3
... 3 Nominal chemical compositions of Group III intermediate-purity ferritic stainless steels UNS No. Alloy designation Composition (a) , wt% C N Cr Mo Ni Ti S44626 26–1 Ti 0.02 (b) 0.025 (b) 26 (b) 1 (b) 0.25 (b) 0.5 (b) S44400 AISI 444 0.02 (b) 0.02 (b) 18...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.9781627082860
EISBN: 978-1-62708-286-0
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320217
EISBN: 978-1-62708-332-4
..., CD4MCu, CF3, CF 3M, CF 8, CF 8M, CF 16F, CG 8M, CH 20, CK 20, CN 7M 2.08 0.25 Corrosion-resistant steels CF 8 C 2.83 0.34 Heat-resistant steels HN, HX 2.33 0.28 Heat-resistant steels HL, HP, HT, HU 2.58 0.31 Heat-resistant steels HK, HN 2.83 0.34 Source: Ref 20 . Courtesy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090067
EISBN: 978-1-62708-266-2
... composition of high-strength steels Type or designation Composition, % C Cr Ni Mo Mn Co Cu Al Ti Si V Nb Low-alloy martensitic 4130 0.30 1.0 … 0.2 0.5 … … … … 0.3 … … 4340 0.40 0.8 1.9 0.25 0.7 … … … … 0.6 … … D6AC 0.45 1.15 0.55 1.0 0.8...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310109
EISBN: 978-1-62708-286-0
... listed in Table 1 with their compositions. Ferritic stainless compositions Table 1 Ferritic stainless compositions Alloy Designation C N Cr Ni Mn Si Mo P S Ti Nb Other 405 S40500 0.08 … 11.5–14.5 0.6 1 1 … 0.04 0.03 … … 0.10–0.30 Al 400 AK alloy 0.05...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080097
EISBN: 978-1-62708-304-1
... ). Resistance to carburization is an important factor in the performance of pyrolysis furnace tubes as well as pigtails for ethylene and olefin plants. Furnace tubes are typically constructed of Fe-Ni-Cr cast alloys, such as HK (Fe-25Cr-20Ni or 25/20), HP (Fe-25Cr-35Ni or 25/35) and their variants. Some...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.9781627082532
EISBN: 978-1-62708-253-2
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930365
EISBN: 978-1-62708-359-1
.... (a) Chilled and white cast irons Welding not recommended Corrosion-resistant cast irons (high Si, high Cr, high Ni) and heat-resistant cast irons Welding confined to minor repair of castings subject to availability of filler materials. For more extensive welding properties of material should...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.t67320033
EISBN: 978-1-62708-347-8
...Chemical compositions of frequently used carburizing grade gear steels, % Table 5.1(a) Chemical compositions of frequently used carburizing grade gear steels, % Material (AISI) C Mn P S Si Ni Cr Mo V W Co 3310 0.08–0.13 0.45–0.60 0.025 max. 0.025 max. 0.20–0.35 3.25...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490265
EISBN: 978-1-62708-340-9
... ( Ref 121 ). Fig. 6.3. HP-IP rotor configurations and cracking locations. (a) Radial-axial bore crack. (b) Transverse crack in heat groove. (c) Creep cracking in blade-attachment area. Fig. 6.40. Effect of hold time on fatigue-crack-growth-rate properties of 2¼Cr-1Mo cast steel ( Ref...