1-20 of 98 Search Results for

Gun tubes

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460107
EISBN: 978-1-62708-285-3
... diameter spray head and adapter are shown in Fig. 4.6 and 4.7 . A new heater design without a preheater and without a hot gas tube makes robotic handling of the gun much more flexible and avoids damage (of the hot gas tube). A new ceramic spray nozzle is distinguished by very good high-temperature...
Image
Published: 01 April 2013
Fig. 6 Test head of the eddy current inspection unit shown in Fig. 5 ; A, orifice for test pipe or tube; B, one of eight paint spray guns for marking; C, reference standard test piece. Source: Ref 1 More
Image
Published: 01 April 2013
Fig. 5 Unit used for the probe type eddy current inspection of seamless steel tubing; A, outer cover, containing test head, in open position; B, one of four rotating eddy current probe coils; C, reference standard test piece in position for calibration; D, one of eight paint spray guns More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720345
EISBN: 978-1-62708-305-8
... is identified by markers. In Fig. 6 , the test head is shown ready for use, with eight paint spray guns in position for marking the proper zone. Fig. 5 Unit used for the probe type eddy current inspection of seamless steel tubing; A, outer cover, containing test head, in open position; B, one of four...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290079
EISBN: 978-1-62708-306-5
..., is called a power/control system. It can weld studs with diameters up to 28.5 mm (1.1 in.). Either a single gun or dual guns can be used. Although a light-duty control system can weigh 11.3 kg (25 lb), the system shown in Fig. 4.3 weighs approximately 450 kg (1000 lb) and can be put on a wheeled cart...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290023
EISBN: 978-1-62708-306-5
... to the electrode through a copper alloy contact tube. The contact tubes have various hole sizes, corresponding to the diameter of the electrode wire. The gun also has a gas-supply connection and a nozzle to direct the shielding gas around the arc and weld pool. To prevent overheating of the welding gun, cooling...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080359
EISBN: 978-1-62708-304-1
... into the boiler through liquor guns at about 4.6 m (15 ft) above the hearth for some boilers ( Ref 6 ). Air for combustion is injected into the furnace separately from primary and secondary air ports for substoichiometric combustion and also from tertiary air ports to complete the combustion. Figure 13.1 shows...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220281
EISBN: 978-1-62708-341-6
..., each tube rests on a rolling cart which proceeds through a long oven. The cart contains its own vacuum pumping system which exhausts the air in the tube as it proceeds through the oven. The cart also carries a work coil which surrounds the electron-gun structure in the tube. This coil is connected...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 May 2018
DOI: 10.31399/asm.tb.hma.t59250187
EISBN: 978-1-62708-287-7
... imported from England and Germany due to a lack of domestic manufacturers. Bethlehem Steel was soon recognized as a producer of ship propeller shafts, large gun barrels, and heavy battleship armor equal to any provided from overseas. The principals put the company up for sale after the turn of the 19th...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460227
EISBN: 978-1-62708-285-3
... temperatures greater than 500 °C (930 °F). Almost all of the high-pressure systems are designed to be used with a stationary robot. These systems typically have spray guns (nozzles and prechamber) that are too heavy to be held by hand. The maximum operating pressure for an HPCS system is 6.9 MPa (1000 psi...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430107
EISBN: 978-1-62708-253-2
... Abstract This chapter describes some of the most effective tools for investigating boiler tube failures, including scanning electron microscopy, optical emission spectroscopy, atomic absorption spectroscopy, x-ray fluorescence spectroscopy, x-ray diffraction, and x-ray photoelectron...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.9781627082532
EISBN: 978-1-62708-253-2
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390241
EISBN: 978-1-62708-459-8
... Abstract Drawing is a bulk deformation process that involves significant surface generation and high pressures. This chapter provides an overview of the mechanics and tribology of wire, bar, tube, and shape drawing. It presents important equations for calculating stresses, forces, friction...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220001
EISBN: 978-1-62708-341-6
..., pins, links, and sprockets could be hardened in large quantities most effectively by high-frequency induction. In a different area, induction heating was applied to preheating of steel blanks prior to hot forging of parts such as gun barrels. In recent years, the application of induction heating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980323
EISBN: 978-1-62708-342-3
... Abstract The machinery and equipment required for rod and tube extrusion is determined by the specific extrusion process. This chapter provides a detailed description of the design requirements and principles of machinery and equipment for direct and indirect hot extrusion. It then covers...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.tt2.t51060251
EISBN: 978-1-62708-355-3
... are obtained from the displacement derivatives, thus: (Eq 8) ε x ≠ 0 , ε y = ε z = 0 The flat plate impact test is performed by launching a flat flyer plate against a second stationary target plate. Compressed gas guns, propellant guns, magnetic accelerators, and explosives...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.9781627083041
EISBN: 978-1-62708-304-1
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2010
DOI: 10.31399/asm.tb.hss.t52790017
EISBN: 978-1-62708-356-0
... and 0.24% carbon. It seems that the alloy did not show the desired improvement with regard to the gun barrels; however, material from the same cast was eventually made into cutlery blades. This, then, was the first commercial cast of what was subsequently known as stainless steel. Fig. 3 Harry...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030292
EISBN: 978-1-62708-282-2
... corrosion resistance, these are often overlaid with stainless steels such as type 347. Other applications for low-alloy steels are furnace tubes, heat-exchangers shells, piping, and separator drums. Stainless Steels Stainless steels are extensively used in petrochemical plants because of the highly...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060175
EISBN: 978-1-62708-261-7
... Hot-rolled alloy steel bars Regular quality Aircraft quality or steel subject to magnetic particle inspection Axle shaft quality Bearing quality Cold-heading quality Special cold-heading quality Rifle barrel quality, gun quality, shell or A.P. shot quality Alloy steel wire Aircraft...