1-20 of 165 Search Results for

Filler metal

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080445
EISBN: 978-1-62708-304-1
... alloys; and iron-, nickel- and cobalt-base filler metals. cast corrosion resistant alloys cast nickel alloys chemical composition cobalt-base alloys filler metals heat-resistant alloys nickel alloys oxide-dispersion-strengthened alloys wrought iron alloys wrought stainless steel...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290165
EISBN: 978-1-62708-306-5
... Abstract Brazing and soldering processes use a molten filler metal to wet the mating surfaces of a joint, with or without the aid of a fluxing agent, leading to the formation of a metallurgical bond between the filler and the respective components. This chapter discusses the characteristics...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120065
EISBN: 978-1-62708-269-3
... the need for contaminant-free surfaces and atmospheres. It describes common forms of fusion, arc, and solid-state welding along with the use of filler metals, shielding gases, and stress-relief treatments. It also discusses the practice of titanium brazing and the role of filler metals. arc...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280149
EISBN: 978-1-62708-267-9
... welding techniques, defect prevention, fixturing, heat treatments, and general practices, including the use of filler metals. It also discusses several solid-state welding methods, superplastic forming, and transient liquid phase bonding, a type of diffusion welding process. The chapter includes extensive...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290137
EISBN: 978-1-62708-306-5
... Abstract Solid-state welding processes are those that produce coalescence of the faying surfaces at temperatures below the melting point of the base metals being joined without the addition of brazing or solder filler metal. This chapter discusses solid-state welding processes such as diffusion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720411
EISBN: 978-1-62708-305-8
... metals and the types of flaws exhibited by brazed joints. brazed joints brazing filler metals eddy current inspection liquid penetrant inspection magnetic particle inspection nondestructive inspection radiographic inspection ultrasonic inspection visual inspection welding weldments...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060117
EISBN: 978-1-62708-261-7
... joining by primary (e.g., metallic) bonds. Unlike welding, however, brazing and soldering do not require or cause any melting (or solid-state mixing of atoms) between the base materials. Rather, bond formation occurs between molten filler and the substrates. Table 6.7 Comparisons of common joining...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170550
EISBN: 978-1-62708-297-6
... filler metal alloys is described by various standards, most notably American Society of Mechanical Engineers (ASME) SFA5.8 and American Welding Society (AWS) A5.8, which give alloy designations in the form BAg- x These alloys are characterized by low melting temperatures and the ability to wet the solid...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080097
EISBN: 978-1-62708-304-1
... Abstract This chapter discusses the conditions under which carburization and metal dusting occur. It describes the chemical reactions and thermodynamic relationships that drive carburization and metal dusting attack and the factors that determine the amount of damage that metals and alloys are...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.9781627083164
EISBN: 978-1-62708-316-4
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240607
EISBN: 978-1-62708-251-8
... Abstract Metal-matrix composites (MMCs) work at higher temperatures than their base metal counterparts and can be engineered for improved strength, stiffness, thermal conductivity, abrasion and/or creep resistance, and dimensional stability. This chapter examines the properties, compositions...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870179
EISBN: 978-1-62708-299-0
... metallic vacuum bag. Fig. 5 Cross section of a continuous-fiber silicon carbide/aluminum composite Discontinuous reinforced aluminum MMCs are produced primarily by casting or P/M processing. In the stir (vortex/mixing) casting process, the pretreated and prepared reinforcement filler phase is...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870537
EISBN: 978-1-62708-314-0
... Abstract This chapter discusses the advantages and disadvantages of metal matrix composites and the methods used to produce them. It begins with a review of the composition and properties of aluminum matrix composites. It then describes discontinuous composite processing methods, including stir...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550457
EISBN: 978-1-62708-307-2
... Abstract Metal-matrix composites can operate at higher temperatures than their base metal counterparts and, unlike polymer-matrix composites, are nonflammable, do not outgas in a vacuum, and resist attack by solvents and fuels. They can also be tailored to provide greater strength and...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550325
EISBN: 978-1-62708-307-2
... Abstract This chapter describes the molecular structures and chemical reactions associated with the production of thermoset and thermoplastic components. It compares and contrasts the mechanical properties of engineering plastics with those of metals, and explains how fillers and reinforcements...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290035
EISBN: 978-1-62708-319-5
... Abstract Generally, binders consist of at least three ingredients: a backbone to provide strength (compounds such as polyethylene, polypropylene, ethylene vinyl acetate, and polystyrene); a filler, such as polyacetal and paraffin wax, to occupy space between particles; and additives, such as...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290023
EISBN: 978-1-62708-306-5
... applies to a large and diversified group of welding processes that use an electric arc as the source of heat to melt and join metals. The formation of a weld between metals that are arc welded may or may not require the use of a filler metal. The welding arc is struck between the workpiece and the tip of...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240597
EISBN: 978-1-62708-251-8
... containing copper (e.g., Ag-10Cu) are traditional coinage alloys. Silver-base brazing filler metal alloys are characterized by low melting temperatures and their ability to wet solid base metals; they are used for brazing steel, cast iron, stainless steel, and copper alloys. They are also used to braze...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910021
EISBN: 978-1-62708-250-1
... Abstract This chapter addresses the basic concepts important to understanding corrosion of metals. It begins with an overview of the three types of behaviors that a metal exhibits when immersed in an environment and of the four requirements of a corrosion cell. The chapter then covers the...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290279
EISBN: 978-1-62708-306-5
... the joint should be considered. However, when dissimilar metals are joined by fusion welding processes, alloying between the base metals and a filler metal, when used, becomes a major consideration. The resulting weld metal can behave much differently from one or both base metals during subsequent...