1-20 of 33 Search Results for

Ferralium

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 June 2008
Fig. 23.10 Duplex microstructure of alloy 255 (Ferralium). Ferrite-dark, austenite-light. Source: Ref 6 More
Image
Published: 01 December 2015
Fig. 43 Preferential corrosion of the ferrite phase in the weld metal of Ferralium alloy 255 gas tungsten arc welds in 10% FeCl 3 at room temperature. Base metal was 3.2 mm (1/8 in.) thick. More
Image
Published: 01 December 2006
Fig. 11 Preferential corrosion of the ferrite phase in the weld metal of Ferralium alloy 255 gas tungsten arc welds in 10% FeCl 3 at room temperature. Base metal was 3.2 mm (⅛ in.) thick. More
Image
Published: 01 December 2015
Fig. 42 Effect of welding heat input on the corrosion resistance of autogenous gas tungsten arc welds in Ferralium alloy 255 in 10% FeCl 3 at 10 °C (40 °F). The base metal was 25 mm (1 in.) thick. Source: Ref 16 More
Image
Published: 01 December 2006
Fig. 10 Effect of welding heat input on the corrosion resistance of autogenous gas tungsten arc welds in Ferralium alloy 255 in 10% FeCl 3 at 10 °C (40 °F). The base metal was 25 mm (1 in.) thick. Source: Ref 20 More
Image
Published: 01 December 2006
Fig. 12 Preferential attack of the continuous austenite phase in an autogenous gas tungsten arc weld in Ferralium alloy 255. Crevice corrosion test was performed in synthetic seawater according to ASTM D 1141 at 100 °C (212 °F). Etched with 50% HNO 3 . 100× More
Image
Published: 01 December 2015
Fig. 44 Preferential attack of the continuous austenite phase in an autogenous gas tungsten arc weld in Ferralium alloy 255. Crevice corrosion test was performed in synthetic seawater according to ASTM D 1141 ( Ref 17 ) at 100 °C (212 °F). Etched with 50% HNO3. 100× More
Image
Published: 01 July 2000
Fig. 7.22 Correlation between the critical pitting temperature and critical pitting potential of 17 high-performance alloys. The alloys are: (1) 317LM, (2) 3RE60, (3) AF22, (4) 44LN, (5) FERRALIUM ALLOY 255, (6) 20CB-3 Alloy, (7) URANUS 86, (8) 2545LX, (9) JESSOP 700, (10) JESSOP 777, (11 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820099
EISBN: 978-1-62708-339-3
... crevice temperature in 10% FeCl 3 · 6H 2 O; pH = 1;24 h exposure °C °F Duplex grades S32900 Type 329 5 41 S31200 44LN 5 41 S31260 DP-3 10 50 S32950 7-Mo PLUS 15 60 S31803 2205 17.5 63.5 S32250 Ferralium 255 22.5 72.5 Austenitic grades S30400 Type...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080443
EISBN: 978-1-62708-304-1
... Elgiloy Company DISCALOY British Steel Corporation E-BRITE U.K. Atomic Energy ELGILOY Bonar Langley Alloys, Ltd. ESSHETE United Technology Corporation FECRALLOY Haynes International, Inc. FERRALIUM Haynes International, Inc. GATORIZE Colt Industries, Inc. G-30, G-35, G-50 Allegheny Ludlum Corporation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030096
EISBN: 978-1-62708-282-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030176
EISBN: 978-1-62708-282-2
... steels with a large numerical value of PREN are the superaustenitics, such as 254SMO (S31254), AL6XN (N08367), 925hMo (N08925), and 654SMO (S32654); the superferritics, such as 29-4C (S44735), Sea-Cure (S44660), and Monit (S44635); and the superduplexes, such as DP-3W (S39274), Ferralium 255 (S32550...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2010
DOI: 10.31399/asm.tb.hss.t52790241
EISBN: 978-1-62708-356-0
...” followed by five digits. For type 304 stainless steel, the UNS number is S30400, and for type 304L, the UNS equivalent is S30403. The system also permits the numbering of stainless steel alloys for which there is no AISI designation, such as S35500 for stainless alloy AM 355. For Ferralium 255, the UNS...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090095
EISBN: 978-1-62708-266-2
... P P 20Mo-6 F P P AISI type 409 P (c) P P Type 439 P P P AISI type 444 P P P E-Brite P P P Sea-Cure F P P Monit F P P AL 29-4 P P P AL 29-4-2 F P P AL 29-4C P P P 3RE60 F NT (e) NT 2205 F NT (P or F) (f) Ferralium F NT...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240433
EISBN: 978-1-62708-251-8
... grades, and superior chloride SCC resistance and pitting resistance. Fig. 23.10 Duplex microstructure of alloy 255 (Ferralium). Ferrite-dark, austenite-light. Source: Ref 6 Composition of duplex stainless steels Table 23.7 Composition of duplex stainless steels Type Composition...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310091
EISBN: 978-1-62708-286-0
... 25 290 30 40 S32001 19D 450 640 25 290 25 … S32101 2101 450 650 25 290 32 40 S32205 2205(new) 460 640 25 290 32 40 S32304 2304 400 600 25 290 31 40 S32520 Uranus 52N+ 550 770 25 … 28 … S32550 Ferralium 550 760 15 302 32 … S32750 2507...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440175
EISBN: 978-1-62708-262-4
...) S31803 SAF 2205 1020–1100 (1870–2010) S31260 DP-3 1065–1175 (1950–2150) S32550 Ferralium 255 1065–1175 (1950–2150) (a) Cooling from the annealing temperature must be rapid, but it also must be consistent with limitations of distortion. Source: Ref 2 Martensitic Grades...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080445
EISBN: 978-1-62708-304-1
... S31803 0.03 (a) 21.0–23.0 4.5–6.5 Bal Mo: 2.5–3.5, N: 0.08–0.2 FERRALIUM 255 S32550 0.04 (a) 24.0–27.0 4.5–6.5 Bal Mo: 2.0–4.0, Cu: 1.4–2.5, N: 0.1–0.25 7-Mo: PLUS S32950 0.03 (a) 26.0–29.0 3.5–5.2 Bal Mo: 1.0–2.5, N: 0.15–0.35 SUPEER-FERRIT … … 28.0 3.2 Bal Mo: 2.1...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170257
EISBN: 978-1-62708-297-6
..., Method B) for a number of commercial duplex stainless steels Stainless steel Cr,% Ni,% Mo,% N,% (max) CCT (°C) Type 329 26 4.5 1.5 — 5 44 LN 25 6 1.7 0.2 5 DP-3 25 7 3 0.3 10 7-Mo Plus 26.5 4.8 1.5 0.35 15 2205 22 5 3 0.2 17.5 Ferralium 255 25 6 3...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410579
EISBN: 978-1-62708-265-5