... has caused local melting, producing pockets of fusion mixtures of iron and aluminum along the interface (marked “A” in Fig. 11.14b ) and within the vortices (marked “B” in Fig. 11.14c ); the composition of region A was about 23% Fe and 77% Al, and that of region B was about 48% Fe and 52% Al. Region...