Skip Nav Destination
Close Modal
Search Results for
FSX 414 (cast cobalt-base superalloy)
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-15 of 15 Search Results for
FSX 414 (cast cobalt-base superalloy)
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170540
EISBN: 978-1-62708-297-6
... is enhanced in these alloys by nickel, which decreases the fcc/hcp transformation temperature in cobalt-base alloys. Cast Heat Resistant Alloys Cast heat resistant alloys, such as alloys MAR-509, FSX-414, and the others listed in Table 5 , are designed around a cobalt-chromium matrix with chromium...
Abstract
This article discusses the properties, behaviors, and uses of cobalt and its alloys. It explains how cobalt alloys are categorized and describes the commercial designations and grades that are available. It also provides composition information and explains how alloying elements and carbides affect toughness, hardness, ductility, and strength as well as resistance to heat, corrosion, and wear.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000117
EISBN: 978-1-62708-313-3
... temperatures up to 400 °C (750 °F). Source: Ref 1 – 16 Selected cobalt cast superalloy compositions Table A.2A Selected cobalt cast superalloy compositions Composition wt% Alloy Fe Co Ni Al Ti Cr Mo W Nb Ta Re B C Zr Y Si Mn AiResist 215 0.5 63 0.5 4.3 … 19...
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280011
EISBN: 978-1-62708-267-9
... Abstract This chapter provides basic materials selection information for iron-nickel-, nickel-, and cobalt-base superalloys. It discusses mechanical and physical properties, the effect of service temperature, and the comparative strengths of wrought and cast product forms. It includes several...
Abstract
This chapter provides basic materials selection information for iron-nickel-, nickel-, and cobalt-base superalloys. It discusses mechanical and physical properties, the effect of service temperature, and the comparative strengths of wrought and cast product forms. It includes several large data tables along with reference information and a detailed application example based on the design of a gas turbine disk.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280001
EISBN: 978-1-62708-267-9
... 3 3.5 5 3 Ta W Zr Other 4.8 6 . . . 0.5 Nb, 0.15 Hf 3 10 . . . 7 5 7 9.25 5 6.5 . . . . . . 1.5 0.08 . . . . . . . . . 0.09 . . . . . . 20 1.5 . . . Superalloys for High Temperatures a Primer / 7 Cobalt-base AiResist 13 AiResist 213 AiResist 215 FSX-414 Haynes 21 Haynes 25; L-605 J-1650 MAR-M 302...
Abstract
This chapter provides a brief introduction to superalloys and their high-temperature capabilities. It explains how and why they were developed and highlights some of their unique properties, behaviors, and characteristics. It discusses their basic metallurgy, how they are processed, and where they are typically used. It also includes nominal composition data for more than 120 superalloys and a concise overview of the major topics in the book.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170290
EISBN: 978-1-62708-297-6
... with consecutive positions in the periodic table of elements. The iron-nickel-base superalloys are an extension of stainless steel technology and generally are wrought, whereas cobalt- and nickel-base superalloys may be wrought or cast, depending on the application/composition involved. The more highly alloyed...
Abstract
This article discusses the composition, structure, and properties of iron-nickel-, nickel-, and cobalt-base superalloys and the effect of major alloying and trace elements. It describes the primary and secondary roles of each alloying element, the amounts typically used, and the corresponding effect on properties and microstructure. It also covers mechanical alloying and weldability and includes nominal composition data on many wrought and cast superalloys.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000133
EISBN: 978-1-62708-313-3
...) … 125 (18) Cobalt-base HS-21 150 (22) 95 (14) 115 (17) 90 (13) 60 (9) 50 (7) X-40 (HS-31) 180 (26) 140 (20) 130 (19) 105 (15) 75 (11) 55 (8) MAR-M 509 270 (39) 225 (33) 200 (29) 140 (20) 115 (17) 90 (13) FSX-414 150 (22) 115 (17) 110 (16) 85 (12) 55 (8) 35 (5...
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280211
EISBN: 978-1-62708-267-9
...) in cast cobalt-base superalloys is interesting. A somewhat similar morphology of M 23 C 6 , occurring when it is precipitated in cellular form in nickel-base and iron-nickel-base alloys, leads to mechanical-property loss in such alloys, but lamellar eutectic does not seem to degrade cast cobalt-base alloy...
Abstract
This chapter examines the effect of heat treating and other processes on the microstructure-property relationships that occur in superalloys. It discusses precipitation and grain-boundary hardening and how they influence the phases, structures, and properties of various alloys. It explains how the delta phase, which is used to control grain size in IN-718, improves strength and prevents stress-rupture embrittlement. It describes heat treatments for different product forms, discusses the effect of tramp elements on grain-boundary ductility, and explains how section size and test location influence measured properties. It also provides information and data on the physical and mechanical properties of superalloys, particularly tensile strength, creep-rupture, fatigue, and fracture, and discusses related factors such as directionality, porosity, orientation, elongation, and the effect of coating and welding processes.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.9781627082679
EISBN: 978-1-62708-267-9
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490415
EISBN: 978-1-62708-340-9
...) Equivalent to PWA 1455. (c) Udimet 700, Astroloy, and Rene 77 are similar in composition. (d) Equivalent to HS-31. (e) Also referred to as Multimet. (f) Total Nb + Ta content specified. Possible influences of environment on fatigue-crack propagation in cast nickel-base superalloys...
Abstract
Combustion turbines consist of a compressor, a combustor, and a turbine. As commonly configured, the compressor and turbine mount on a single shaft that connects directly to a generator. This chapter reviews the materials of construction, damage mechanisms, and life-assessment techniques for nozzles and buckets. It also presents key information from a detailed review of the literature and the results of a survey on combustion-turbine material problems.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280287
EISBN: 978-1-62708-267-9
... superalloys such as IN-100 and B-1900 nickel-base superalloys. Cobalt-base superalloys did not suffer as much from hot corrosion, owing to high chromium concentrations in such alloys; iron-nickel-base superalloys generally did not operate at temperatures sufficiently high as to encounter hot corrosion...
Abstract
Superalloys tend to operate in environments where they are subjected to high-temperature corrosion, oxidation, and the erosive effects of hot gases. This chapter discusses the nature of these attacks and the effectiveness of various protection methods. It describes the primary forms of oxidation, the development of protective oxides, and the conditions associated with mixed gas corrosion and hot corrosion attack. It discusses oxidation and corrosion testing, the equipment used, and various ways to present the associated data. It describes the effect of gaseous oxidation on different alloys, discusses the formation of oxide scale in the presence of mixed gases, and explains how alloy composition contributes to oxide growth. The chapter discusses the underlying chemistry of hot corrosion, how to identify its effects, and how it progresses under various conditions. It also discusses protective coatings, including aluminide diffusion, overlay, and thermal barrier types, and how they perform in different environments based on their ability to tolerate strain.
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310351
EISBN: 978-1-62708-326-3
... to improve the fluidity during casting, is thus an alloying constituent in casting alloys. The commercial heat treatable aluminum alloys are, with few exceptions, based on ternary or quaternary systems with respect to the solutes involved in developing strength by precipitation. Commercial alloys whose...
Abstract
The term heat treatable alloys is used in reference to alloys that can be hardened by heat treatment, and this chapter briefly describes the major types of heat treatable nonferrous alloys. The discussion provides a general description of annealing cold-worked metals and describes some of the common nonferrous alloys that can be hardened through heat treatment. The nonferrous alloys covered include aluminum alloys, cobalt alloys, copper alloys, magnesium alloys, nickel alloys, and titanium alloys.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.9781627082976
EISBN: 978-1-62708-297-6
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030025
EISBN: 978-1-62708-282-2
... illustrates the morphology of a semiprotective scale formed on a cobalt-chromium alloy. Alloys based on these minimum specifications will form the desired protective oxide upon initial exposure, but because of the accompanying depletion of the scale-forming element, they will probably be unable to re-form...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.9781627083409
EISBN: 978-1-62708-340-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.9781627083041
EISBN: 978-1-62708-304-1