1-20 of 320 Search Results for

Engine cylinders

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 January 2022
Fig. 11.18 Engine cylinder block cast using the SinterCast process. Source: Ref 8 . Courtesy of SinterCast More
Image
Published: 01 January 2022
Fig. 6.14 Diesel engine cylinder block pouring. Source: Ref 3 More
Image
Published: 01 January 2022
Fig. 3.8 Air cooled engine cylinder head More
Image
Published: 01 January 2022
Fig. 7.35 Cut section of a marine diesel engine cylinder block More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270172
EISBN: 978-1-62708-301-0
... Abstract During a routine preflight inspection of a piston aircraft engine, part of a cooling fin was found that had broken off the cylinder. The piece, made of aluminum-silicon alloy, was cleaned and examined. Based on the fracture characteristics revealed by an electron microscope...
Image
Published: 30 November 2013
Fig. 11 Cavitation pitting fatigue. (a) Cavitation pitting on a gray cast iron diesel-engine cylinder sleeve. The pitted area is several inches long, and the pits nearly penetrated the thickness of the sleeve. Note the clustered appearance of the pits at preferred locations. (b) Cavitation More
Image
Published: 01 November 2012
Fig. 25 Cavitation pitting fatigue. (a) Cavitation pitting on a gray cast iron diesel engine cylinder sleeve. The pitted area is several inches long, and the pits nearly penetrated the thickness of the sleeve. Note the clustered appearance of the pits at preferred locations. (b) Cavitation More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320207
EISBN: 978-1-62708-332-4
... engine cylinder blocks, exhaust manifolds, and heavy-duty brake rotors. Compacted graphite iron is also known as vermicular graphite iron . The network of graphite flakes in cast iron imparts high thermal-conductivity properties. However, the sharp edges of the graphite flakes act as stress risers...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410001
EISBN: 978-1-62708-280-8
... Brake master cylinders Brake calipers ABS housings Corrosion resistance Advantages include: Minimum property deterioration with time Reduced maintenance costs Improved aesthetic appeal Anodizing and clear coating can enhance corrosion resistance. Marine engine propeller Aluminum...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320305
EISBN: 978-1-62708-332-4
... is needed for wider implementation. Downsized engines in cast iron, compacted graphite iron (CGI), or aluminum for HEVs and PHEVs are placed in the front hood. The number of engine cylinders commonly range from two to three, although four-cylinder engines are also designed. Reference 4 illustrates...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.9781627083324
EISBN: 978-1-62708-332-4
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270175
EISBN: 978-1-62708-301-0
... Abstract Several hydraulic pumps that failed in service on a particular type of aircraft were received for analysis. Hydraulic testing was not an option, so the pumps were disassembled and their plungers and cylinders were cleaned and examined. Based on their observations, investigators...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320103
EISBN: 978-1-62708-332-4
.... Gray iron’s heat conduction and heat- and wear-resistance properties make it uniquely suitable for automotive engine cylinder blocks, cylinder liners, disc brake rotors and brake drums, air compressor cylinder blocks, and paper-making drying cylinders. Special properties such as corrosion resistance...
Image
Published: 01 December 1995
Fig. 2-158 Non-magnetic (austenitic stainless steel) cylinder castings for a diesel engine which powers a mine sweeper. Weights 35 to 150 lb (16 to 68 kg) More
Image
Published: 01 October 2011
Fig. 5.26 Examples of aluminum permanent castings: control arm, brake master cylinders and calipers, steering knuckles, valve housing, and engine mounting brackets. Courtesy of General Aluminum Manufacturing Co. More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400203
EISBN: 978-1-62708-316-4
... in the process design stage. The Engineering Research Center for Net Shape Manufacturing, as part of an USCAR project, developed an optimization methodology coupled with commercial finite element codes to estimate the BHF for individual cylinders in MPC systems ( Fig. 13.28 , 13.29 ) ( Ref 13.1 ). Fig...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410151
EISBN: 978-1-62708-280-8
... Brake calipers, brake master cylinders, ABS bodies Engine cylinder heads, cylinder blocks, crank cases, oil pans, differential carriers, engine front covers, intake manifolds, water pump bodies, oil line adapters, air conditioning compressor bodies and supercharger rotors, pistons, marine propellers...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300179
EISBN: 978-1-62708-323-2
... combustion engines. The graphite flakes are thought to act as oil reservoirs to help maintain the hydrodynamic film separation of piston rings and cylinder liners. Ductile irons contain alloy elements such as magnesium to make the graphite form into spherical shapes on cooling. This increases...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460209
EISBN: 978-1-62708-285-3
.... , and Verpoort C. , A Materials System and Method of Its Application for the Wear Protection of Aluminum Engine Cylinder Bore Surfaces , Proc. 2004 International Thermal Spray Conference , 2004 8.30 Barbezat G. , Advanced Thermal Spray Technology and Coating for Lightweight Engine Blocks...
Book Chapter

By Eren Billur
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400181
EISBN: 978-1-62708-316-4
.... hydraulic drive systems hydraulic press HYDRAULIC PRESSES generate the forming force and necessary ram motion by hydraulic cylinders. The pressurized fluid medium drives the piston in the cylinder, and the motion is controlled using a set of valves. A typical hydraulic circuit consists of a reservoir...