Published: 01 November 2013
Fig. 5 Electroplating setup More
Image
Published: 01 December 2000
Fig. 11.5 Processing sequence for electroplating copper on titanium alloy parts Solution No. Type of solution (a) Composition of solution 1 Acid dip 60% HF, 1 vol, 69% HNO 3 , 3 vol 2 Dichromate dip Na 2 Cr 3 O 7 · 2H 2 O, 290 g/L (39 oz/gal), 60% HF, 55 g/L (7.3 oz/gal More
Image
Published: 01 April 2004
Fig. 4.2 A porous ceramic material metallized with a thick silver electroplate. The residual stress in the metallization has resulted in a peel failure through the near-surface layer of the ceramic. More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230361
EISBN: 978-1-62708-298-3
... Abstract This chapter discusses coating technologies that are applicable to beryllium, including physical and chemical vapor deposition, thermal evaporation, electroplating, sputtering, ion plating, and plasma arc spraying. It describes the advantages and disadvantages of each method...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
..., and inspection and quality assurance. The next section discusses the methods by which metals, and in some cases their alloys, can be applied to almost all other metals and alloys: electroplating, electroless plating, hot dipping, thermal spraying, cladding, pack cementation, vapor deposition, ion implantation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870191
EISBN: 978-1-62708-299-0
... the basic factors that influence design for corrosion resistance and discusses the use of conversion coatings, organic coatings, porcelain enameling, and electroplating. It also discusses corrosion monitoring methods used in chemical processing and refining industries. aluminum aluminum alloys...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350183
EISBN: 978-1-62708-315-7
..., uncoated cemented carbide, TiC + TiN by CVD, TiC by CVD, VC by TRD, and NbC by TRD Table 1 Compares the processing characteristics for electroplating, electroless plating, CVD, PVD, thermal diffusion, ion nitriding, TRD, ion implantation, ion-beam assisted deposition, and thermal spraying Table 9...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850538
EISBN: 978-1-62708-260-0
..., gold, beryllium, aluminum, carbon, vanadium, molybdenum, tungsten, chromium, selenium, titanium, and uranium. Cannot be plated . Bismuth, cadmium, tin, lead, and zinc (electroplate with copper, then use electroless nickel). A wide variety of nonmetals such as plastics, wood, glass, carbide...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
... coat, conversion coat, hardface, electroplate, and so on Fig. 12.1 Estimate of the relative use of material modifications to surfaces to (a) lubricate/alter function or appearance and (b) harden surfaces/bulk material. PTFE, polytetrafluoroethylene; PFA, perfluoroalkoxy; DLC, diamond-like...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900163
EISBN: 978-1-62708-350-8
... for gas nitriding: electroplating and paint-on methods. Electroplating One method of selective gas nitriding is to plate the areas to be stopped-off using copper or bronze. Nickel and silver are also effective but costly, restricting their use to special applications. Copper plating is perhaps most...
Image
Published: 01 April 2004
Fig. 5.22 Oxygen concentration at 3 nm (0.1 μin.) depth in the gold surface of solderability reference standard material as a function of the heat treatment condition. The substrate material is nickel sheet, electroplated with 10 μm (390 μin.) nickel, overlaid with 5μm (200 μin.) gold. More
Image
Published: 01 August 2005
of each sheet by electroplating. More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
... overlays, thermal spraying, and various deposition technologies. ceramic coating chemical vapor deposition cladding corrosion resistance electroless plating electroplating hot dip metallic coating physical vapor deposition thermal spraying weld overlays THE SURFACE-ENGINEERING METHODS...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350195
EISBN: 978-1-62708-315-7
... such as polytetrafluoroethylene (PTFE) Fretting Fatigue With high loads or prolonged operation, fretting may lead to crack initiation followed by fretting fatigue. Since electroplating can impair fatigue resistance of the substrate, the best solutions are usually the intrinsically hard and tough thermally sprayed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.t65940451
EISBN: 978-1-62708-302-7
... by the Corrodkote Procedure • B 457, Method for Measurement of Impedance of Anodic Coatings on Aluminum • B 537, Practice for Rating of Electroplated Panels Subjected to Atmospheric Exposure • B 577, Test Methods for Hydrogen Embrittlement of Copper • B 583, Test Methods for Porosity in Gold...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
.... Environmental Regulations Environmental protection regulations are often directly or indirectly related to finishing and coating processes. This is particularly true for solvent cleaning procedures, cadmium and chromium electroplating, chromate conversion coatings, and organic coatings containing high...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350231
EISBN: 978-1-62708-315-7
... treatment involving the enrichment of the surface layer of an object with borides. This surface-hardening process is performed below the Ac1 temperature. Also referred to as boronizing. bright finish. A high-quality finish produced on ground and polished rolls. Suitable for electroplating. bright nitriding...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280203
EISBN: 978-1-62708-267-9
..., discoloration, and soils. Metal loss is not excessive when normal pressures and exposure times are used. Surfaces that have been wet blasted are usually suitable for welding, brazing, electroplating, and final inspection; further cleaning is seldom necessary. Exceptions are the precipitation-hardened nickel...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030165
EISBN: 978-1-62708-282-2
... a barrier between the metal substrate and the environment. In addition, metallic coatings can sometimes provide cathodic protection when the coating is compromised. Metallic coatings and other inorganic coatings are produced using a variety of techniques, including hot dipping, electroplating, cladding...