1-20 of 474 Search Results for

Die castings

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410103
EISBN: 978-1-62708-280-8
... Abstract The die casting process is a widely applied technique used by a variety of industries. This chapter reviews the casting design and engineering requirements for optimizing the characteristics of die castings. die castings casting design The die casting process is a widely...
Image
Published: 01 October 2011
Fig. 5.27 Typical high-pressure die castings. Courtesy of North America Die Casting Association More
Image
Published: 30 June 2023
Fig. 16.18 Aluminum die castings used to fasten curtain wall panels. More
Image
Published: 30 November 2023
Fig. 8.1 Typical die castings (a) steering gear, (b) transmission valves ( Ref 1 ), (c) engine cylinder block ( Ref 2 ) More
Image
Published: 01 December 2018
Fig. 4.34 Schematic for producing rapid die castings More
Image
Published: 30 April 2021
Fig. 9.23 Ice cream scoop made from zinc die castings More
Image
Published: 01 December 1995
Fig. 13-19 Steel die castings More
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370167
EISBN: 978-1-62708-447-5
... Abstract This chapter provides an overview of aluminum die casting and the equipment used. It discusses the advantages and limitations of the die casting process and the design and operation of hot- and cold-chamber die casting machines. It also discusses clamping systems and forces...
Image
Published: 01 November 2013
Fig. 29 Components of a single-cavity die casting die for use in a hot chamber machine. Source: Ref 6 More
Image
Published: 01 December 2004
Fig. D6.86 360.0-F, die cast aluminum casting rotating-beam fatigue curve. Smooth specimens from one lot More
Image
Published: 01 December 2004
Fig. D6.87 A360.0-F, die cast aluminum casting rotating-beam fatigue curve. Smooth specimens from one lot More
Image
Published: 01 December 2004
Fig. D6.88 364.0-F, die cast aluminum casting rotating-beam fatigue curve. Smooth specimens from two lots. Specimen per Fig. A3.4, Appendix 3 . Data points with lines indicate failures near fillet radius. More
Image
Published: 01 December 2004
Fig. D6.89 380.0-F, die cast aluminum casting rotating-beam fatigue curve. Smooth specimens from one lot. Specimen per Fig. A3.4, Appendix 3 . More
Image
Published: 01 December 2004
Fig. D6.90 380.0-F, die cast aluminum casting rotating-beam fatigue curve. Smooth specimens from one lot. Specimen per Fig. A3.4, Appendix 3 , as cast. Machined to nominal diameters as noted More
Image
Published: 01 December 2004
Fig. D6.91 380.0-F, die cast aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from one lot. Notched specimens similar to Fig. A3.2(b), Appendix 3 , except notch radius is as noted More
Image
Published: 01 December 2004
Fig. D6.92 A380.0-F, die cast aluminum casting rotating-beam fatigue curve. Smooth specimens from one lot More
Image
Published: 01 December 2004
Fig. D6.93 384.0-F, die cast aluminum casting rotating-beam fatigue curve. Smooth specimens from one lot More
Image
Published: 01 December 2004
Fig. D6.94 390.0-F, die cast aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from one lot. Smooth specimens per Fig. A3.7, Appendix 3 . Notched specimens similar to Fig. A3.2(b), Appendix 3 , except notch radius is as noted More
Image
Published: 01 December 2004
Fig. D6.95 413.0-F, die cast aluminum casting rotating-beam fatigue curve. Smooth specimens from one lot More
Image
Published: 01 December 2004
Fig. D6.96 413.0-F, die cast aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from one lot More