... Nickel-iron base Cobalt base Nickel base Solid-solution strengtheners Cr, Mo Nb, Cr, Mo, Ni, W, Ta Co, Cr, Fe, Mo, W, Ta, Re, Al, Ti Face-centered cubic matrix stabilizer C, W, Ni Ni, Fe … Carbide formation:      MC Ti, Nb, Ta Ti, Nb, Ta W, Ta, Ti, Mo, Nb, Hf      M 7 C 3...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080005
EISBN: 978-1-62708-304-1
... , p 187 10.1016/0921-5093(91)90738-9 58. Lai G.Y. , Sulfidation-Resistant Co-Cr-Ni Alloys with Critical Contents of Silicon and Cobalt , U.S. Patent No. 4711763 , Dec 1987 59. Lai G.Y. , Meeting the Challenge of Materials Development for Coal Combustion Plants , Mater...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000025
EISBN: 978-1-62708-313-3
... ( Ref 26 ). In alloys containing hafnium, the formation of (yttrium, hafnium) oxides has been observed ( Ref 21 ). The formation of orthorhombic AlYO 3 (yttrium-aluminum perovskite) and tetragonal Y 3 Al 5 O 12 (yttrium-aluminum garnet) has been observed in the ferritic alloy MA-956 and is shown...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170290
EISBN: 978-1-62708-297-6
... in Fig. 3 . Table 1(a) Common ranges of major alloying additions in superalloys Element Range, % Fe-Ni- and Ni-base Co-base Chromium 5–25 19–30 Molybdenum, tungsten 0–12 0–11 Aluminum 0–6 0–4.5 Titanium 0–6 0–4 Cobalt 0–20 … Nickel … 0–22 Niobium 0–5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280025
EISBN: 978-1-62708-267-9
... 0–12 0–11 Al 0–6 0–4.5 Ti 0–6 0–4 Co 0–20 … Ni … 0–22 Nb 0–5 0–4 Ta 0–12 0–9 Re 0–6 0–2 Table 3.3 Role of alloying elements in superalloys Effect (a) Iron-base Cobalt-base Nickel-base Solid-solution strengtheners Cr, Mo Nb, Cr, Mo, Ni, W...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280287
EISBN: 978-1-62708-267-9
... are alloy elements added in considerable amounts for the purpose of effecting an improvement in the oxidation resistance (chromium) and strength (aluminum) of a superalloy. Oxides of particular interest are: Chromic oxide (Cr 2 O 3 ) Aluminum oxide (Al 2 O 3 ) Nickel oxide (NiO) Cobalt oxide...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240563
EISBN: 978-1-62708-251-8
... is the fcc intermetallic compound Ni 3 (Al,Ti), either in the form of Ni 3 Al or Ni 3 Ti. Other elements, notably niobium, tantalum, and chromium, also enter γ′. In nickel-base alloys, γ′ is typically Ni 3 (Al,Ti), but if cobalt is added, it can substitute for some nickel as (Ni,Co) 3 (Al,Ti). Since the γ...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130541
EISBN: 978-1-62708-284-6
...–64 Wrought magnesium aluminum zinc 80 47 Pure Indium (In) 51–113 30–65 Cast rare earth magnesium alloys 72–92 42–53 Pure Nickel (Ni) 69–99 40–57 Pure Cobalt (Co) 87 50 Pure Osmium (Os) 88 51 Pure Rhodium (Rh) 88 50 Pure Gallium (Ga) 87–91 50–53 Pure Chromium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430027
EISBN: 978-1-62708-253-2
... to stabilize ferrite: Cr, W, Mo, V, and Si Elements that tend to graphitize carbides: Si, Co, Al, and Ni are graphitizers. Their presence makes carbides unstable. Elements that tend to form nitrides: Ti, Al, V, and Zr Elements that remain in a free state: Pb and Cu The alloying...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850165
EISBN: 978-1-62708-260-0
... H. : “ The Development of Metallographic Structures by Solutions, ” Neue Huette , vol. 14 , 1969 , pp. 685 – 690 . 4. Bloor D. W. : “ Etching with Special Reference to Nickel-Chromium-Cobalt Alloys, ” Metallurgia , vol. 66 , no. 395 , 1962 , pp. 139 – 142 . 5. Bloor D...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280117
EISBN: 978-1-62708-267-9
... as-HIP (not forged) P/M superalloys. Table 7.1 Composition of some P/M superalloys Alloy Composition, wt% C Cr Mo W Ta Ti Nb Co Al Hf Zr B Ni Other Rene 95 0.07 13.0 3.5 3.5 … 2.5 3.5 8.0 3.5 … 0.05 0.01 bal … IN-100 0.07 12.5 3.2 … … 4.3 … 18.5...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.9781627082600
EISBN: 978-1-62708-260-0
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980195
EISBN: 978-1-62708-342-3
... spectrum of materials to be extruded. This chapter focuses on the processes involved in the extrusion of semifinished products in various metals and their alloys, namely tin, lead, lead-base soft solders, tin-base soft solders, zinc, magnesium, aluminum, copper, titanium, zirconium, iron, nickel...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740213
EISBN: 978-1-62708-308-9
... for various cutting tool materials. Courtesy Metcut Research Associates, Inc. Source: Ref 8 Cobalt-base cutting tools have been available since about 1920. These materials are generally cast Co-Cr-W alloys with carbon and other alloy additions. They are not heat treatable, and the maximum hardness...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230523
EISBN: 978-1-62708-298-3
... – 506 Beaver W.W. , and Magalski R. , 1953 . Brush Beryllium Corporation , private communication Beaver W.W. , and Stonehouse A.J. , 1963 . “ Beryllium: Surface Treatment and Coatings ,” Report NP-14783, Brush Beryllium Co . Beaver W.W. , et al . , 1964...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.9781627082983
EISBN: 978-1-62708-298-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850060
EISBN: 978-1-62708-260-0
... . 59. Keller F. , and Wilcox G. W. : “ Anodically Oxidized Aluminum Alloys—Metallographic Examination, ” Met. Alloys , vol. 10 , 1939 , pp. 187 – 195 . 60. Atkinson J. T. N. , and Godden C. A. : “ Novel Metallographic Techniques, Particularly as Applied to the Study...