1-20 of 331 Search Results for

Banding

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410163
EISBN: 978-1-62708-265-5
... of segregation and inclusions and their effect on the mechanical properties and microstructure of steel. It explains how to identify various types of inclusions and characteristic segregation patterns, such as banding. It also describes the effect of hot work processing on solidification structure...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560081
EISBN: 978-1-62708-291-4
... banding. It also describes some of the alloying variations that have been developed to improve machinability and the mechanisms by which they work. free-machining inclusions lamellar tearing low-carbon structural steels The next group of steels that we can conveniently distinguish can...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560125
EISBN: 978-1-62708-291-4
... it intermingles with proeutectoid ferrite and cementite. It explains how ferrite and pearlite respond to deformation and how related features such as slip lines, dislocations, shear bands, and kinking can be detected as well as what they reveal. It also describes the structure of patented wires, cast steels...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430107
EISBN: 978-1-62708-253-2
... tube sample Fig. 5.6 Variation in scale thickness on flue gas side of a superheater tube Location Scale thickness, μm 1 583.5 2 575.8 3 524.9 4 675.2 5 537.6 Avg 579.4 Fig. 5.7 Microstructure of steel showing pearlite banding Fig. 5.8...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730037
EISBN: 978-1-62708-283-9
.... It discusses the significance of energy bands, intrinsic and extrinsic conduction, and the properties of compound semiconductors. It also covers semiconductor devices, including p-n junctions, light emitting diodes, transistors, and piezoelectric crystals. electrical behavior light emitting diodes...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220353
EISBN: 978-1-62708-259-4
... rates. It describes special cases of segregation, including banding and why it occurs, and the application of closed die forging. The chapter also presents several examples of hot working defects, including forging laps, cracks, and overheated or burned steel. closed die forging hot working...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860035
EISBN: 978-1-62708-338-6
... Fig. 4.5 Single circuit repeated for axisymmetric coverage Fig. 4.1 Development of band pattern with winding circuits Fig. 4.2 Simple dwell method of pipe winding Fig. 4.3 Advanced method of pipe winding Fig. 4.4 Geodesic path on a curved surface...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860065
EISBN: 978-1-62708-338-6
... Fig. 6.16 Crossing band thickness reduction Fig. 6.17 Filament-wound hole Fig. 6.18 Leakage path between plies Fig. 6.19 Filament winding progressive cure Fig. 6.20 Caul plate and filament-wound surface finish Fig. 6.21 Clay pipe flange Fig...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110180
EISBN: 978-1-62708-247-1
... section discusses the value and application of spectral information in the PE signal. For TRE or PICA, time resolution is an additional requirement. Detector Sensitivity Time Resolution 4.3) Image Resolution Solid Immersion Lens Evaluation of PE Spectra Electron Temperature and Band Gap...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240303
EISBN: 978-1-62708-251-8
... 31.0 248 Zinc 7.133 0.382 39.7 113 59.16 Zirconium 6.505 0.30 5.85 21.1 450 Source: Ref 1 17.1 Density 17.2 Thermal Properties 17.3 Band Theory of Metals 17.4 Electrical Properties 17.5 Magnetic Properties 17.6 Optical Properties Acknowledgments...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140165
EISBN: 978-1-62708-264-8
... solidify a big ingot of steel, powders formed from small liquid droplets freeze very rapidly, thus reducing the dendrite spacing. After compaction and high-temperature sintering, one ends up with much finer primary carbides. The phenomenon of banding in steels discussed in Chapters 4 and 5 ( Fig...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.t60400049
EISBN: 978-1-62708-258-7
.... Fig. 3.48 Microstructure of a cold-drawn and spheroidized AISI/SAE 1095 steel bar showing regions of graphite (elongated, dark bands). 4% picral etch. 1000×. Courtesy of S. Lawrence, Bethlehem Steel’s Homer Research Center The development of graphite in a 1.2% C steel is shown in Fig. 3.49...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410213
EISBN: 978-1-62708-265-5
... is applied. The burst of new dislocations produces a localized strain, referred to as the Lüders strain, that produces a band of plastic deformation, referred to as a Lüders band. The band propagates across the gage length of a tensile specimen, a process shown schematically in Fig. 11.9 ( Ref 11.20...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140201
EISBN: 978-1-62708-264-8
... becomes higher as λ becomes smaller. If the wavelength of the light is restricted to a narrow band of wavelengths in a range that is visible to the human eye, the brain distinguishes, or sees, specific colors. [1] Table A3 lists the bands of wavelengths of the common colors. However, as illustrated...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090333
EISBN: 978-1-62708-266-2
... strength of 2.45 to 3.92 GPa (355 to 569 ksi) and a Young’s modulus of 127 to 166 GPa (18.4 to 24.1 × 10 3 ksi) ( Ref 13.2 ). These alloys are capable of plastic deformation on shear bands, although in tension the plastic elongation to fracture is generally less than 2%. Amorphous alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.9781627083386
EISBN: 978-1-62708-338-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310155
EISBN: 978-1-62708-286-0
... of the entire hot band surface. These tendencies are fought by low oxygen and sulfur levels and minimal slab-reheating temperatures and times, as well as slab surface working in the caster pinch rolls. Sometimes, very poor hot working alloys are given a single hot reduction pass on a hot mill to produce a full...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780404
EISBN: 978-1-62708-281-5
... a polystyrene sample that was deformed past its compressive yield. The section is viewed between cross polars, showing shear bands. 50× Fig. 8 Surface-microcracking network developed on polyoxymethylene due to ultraviolet exposure. 200× Fig. 29 Reflected-light optical micrograph...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780359
EISBN: 978-1-62708-281-5
... the correlation between structure and absorption bands. Lexan, G.E. Plastics Fig. 4 Fourier transform infrared spectral comparison showing distinct differences between the results obtained on various plastic materials Fig. 6 Differential scanning calorimetry used to identify polymeric...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440243
EISBN: 978-1-62708-262-4
... temper to adjust mean to 35 HRC. Source: Ref 1 Fig. 6 Factors contributing to overall heat treating process result variations. Source: Ref 1 Fig. 1 Microstructure of hot-rolled AISI 1022 steel showing severe banding. Bands of pearlite (dark) and ferrite were caused by segragation...