Skip Nav Destination
Close Modal
By
T.J. Eden, D.E. Wolfe, V. Champagne, C. Widener
By
Scott MacKenzie
Search Results for
Axle housings
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 57
Search Results for Axle housings
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Image
Published: 01 January 2022
Image
(a) Fracture surface of a 3.6-in.-diam axle housing tube showing four major...
Available to PurchasePublished: 30 November 2013
Fig. 25 (a) Fracture surface of a 3.6-in.-diam axle housing tube showing four major fatigue-fracture origins (arrows) at the bottom. (b) Origin areas at higher magnification. Beach marks are clearly seen. Small areas of postfracture damage are present, but in general, the fracture
More
Image
Published: 01 December 2004
Image
Published: 01 January 2022
Image
Published: 01 January 2022
Image
Published: 01 January 2022
Image
Published: 01 December 1995
Image
Published: 01 January 2022
Image
Published: 01 December 1995
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.9781627083324
EISBN: 978-1-62708-332-4
Book Chapter
Applications of Iron and Steel Castings and the Impact of Electric Vehicles
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320305
EISBN: 978-1-62708-332-4
.... Components for the refrigeration industry are prime examples. Figure 13.6 presents an overview of the attributes and applications of steel castings. Fig. 13.6 Attributes and applications of steel castings In summary, although some structural components such as axle housings can be replaced...
Abstract
Iron and steel have been the most useful materials to meet the needs of several industries for many decades. Each iron and steel alloy offers unique attributes that make them the best choice for an application. This chapter provides an overview of each ferrous alloy—gray iron, malleable iron, compacted graphite iron (CGI), ductile iron, austempered ductile iron (ADI), and carbon steel and low-alloy steel; its versatile attributes; and its individual applications. A large section of the chapter covers the impact of electric vehicles on the future of the iron and steel castings industry, including discussion on electric vehicle categories and weights; impact of center of gravity on stability and steering; lightweighting incentives; and engineering for improved suspension.
Book Chapter
Aluminum Casting Applications
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410001
EISBN: 978-1-62708-280-8
... Rack and pinion housings Mass reduction Master cylinder Mass reduction ABS housings Mass reduction Body Front cross member Vehicle front-axle mass reduction Middle cross member Body mass reduction Shock towers Body mass reduction A & B pillars Body mass reduction...
Abstract
Casting is one of the most economical manufacturing processes for providing shape to components of machinery and is used in a wide range of industries. This chapter is a brief account of the advantages, applications, limitations, and market growth of aluminum casting. It also provides information on the process of conversion of steel and iron parts to aluminum.
Book Chapter
Engineering Carbon and Alloy Steel Castings
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320217
EISBN: 978-1-62708-332-4
... undercarriage. Source: Ref 4 Fig. 12.10 Bolster casting Typical examples of highway castings are axle housings, differential housings, truck wheel spiders, brake spiders, brake shoes, and spindles. Figure 12.11 ( Ref 5 ) shows an axle housing for a truck with the two arms mounted on either...
Abstract
Steel is broadly classified as plain-carbon steels, low-alloy steels, and high-alloy steels. This chapter begins by describing microconstituents of low- and medium-carbon steel, including bainite and martensite. This is followed by a section discussing the effect of alloying elements on steel. Then, it provides an overview of steel casting applications. Next, the chapter reviews engineering guidelines for steel castings and feeder design. The following section provides information on feeding aids. Further, the chapter describes the elements of gating systems for steel castings. It also describes the alloys, properties, applications, and engineering details of steel. Finally, the chapter explains defects in steel castings and presents guidelines for problem solving with examples.
Book Chapter
Industrial Applications of Steel Castings
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200007
EISBN: 978-1-62708-354-6
.... Fig. 2-17 Trailer hitch, shell molded cast steel. Weight 4.5 lb (2 kg) Fig. 2-18 Cast steel trailer hitch is a 1 lb (0.45 kg) casting An important motor vehicle part is the rear housing for heavy-duty trucks, Figure 2-19 . This axle unit is rugged and lightweight with a thin...
Abstract
Steel castings are produced in thousands of designs for different applications. They fill needs in many industries, including transportation, construction machinery, earthmoving equipment, rolling mills, mining, oil and gas exploration, and power generation. This chapter touches upon the variety of applications for which steel castings can be supplied and the ranges of casting size and complexity. Photographs in this chapter provide an understanding of these applications, their size and complexity, and the types of cast steels produced.
Book Chapter
Cold Spray Applications in the Defense Industry
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460227
EISBN: 978-1-62708-285-3
... of different components made from magnesium and aluminum alloys. Cast magnesium and aluminum alloys are used in aircraft components such as gear boxes and transmission housings because of their light weight, high strength-to-weight ratios, and lower manufacturing costs. The gear boxes and transmission housings...
Abstract
High-pressure cold spray repair process has been used on a number of different applications in the defense industry. This chapter describes various applications for cold spray systems that have operating pressures greater than 2.4 MPa (350 psi) and operating temperatures greater than 500 deg C (930 deg F).
Book Chapter
Influence of Microstructure on Mechanical Properties and Performance
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320031
EISBN: 978-1-62708-332-4
Abstract
This chapter discusses the crystal structures of steel and cast iron, the iron-iron carbide equilibrium diagram, microconstituents or phases in the iron-iron carbide phase diagram, the iron-carbon carbide-silicon equilibrium diagram of cast irons, and the influence on microstructure by base elements and alloying elements. Graphitization, cooling rates, and heat treatment effects are covered. There also is discussion on inoculation benefits, flake graphite types and typical applications, evolution of cast iron types, ASTM specification A247 for graphite shapes, and selection of the best molding process. A large table lists typical material choices for various applications.
Book Chapter
Introduction to Steel Castings
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200001
EISBN: 978-1-62708-354-6
.... in valves and blowout preventers. Heavy trucks—both on and off-highway—use about 5% of industry production. Some applications include: axle housings, suspension brackets, wheels, brake parts, axle spindles, differential housings, and fifth wheels. Mining industry makes extensive use of steel...
Abstract
This chapter defines steel castings, explains when to use steel castings, gives an overview of casting processes, and gives examples of suitable applications for cast steel parts.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040141
EISBN: 978-1-62708-300-3
..., the shape of the die segments on the forging rolls determines the rolled configuration. An example illustrating the application of preforming by roll forging, or reducer rolling, is shown in Fig. 12.3 . Another example, illustrating preforming for a truck axle forging, is seen in Fig. 12.4 . Fig...
Abstract
Prior to forging, it is often necessary to preform billet stock to achieve adequate material distribution. This chapter discusses the equipment used for such operations, including transverse rolling machines, electric upsetters, ring-rolling mills, horizontal presses, and rotary (orbital) and radial forging machines. It describes their basic operating principles as well as advantages and disadvantages.
Book Chapter
Engineering Ductile Iron Castings
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320163
EISBN: 978-1-62708-332-4
... Product application Automotive Suspension components such as front and rear knuckles and control arms, brake calipers, crank-shafts, cam shafts, exhaust manifolds, wheel hubs, balance shafts, gears, bushings, flanges, brackets Off-highway and class eight trucks Axle housings, differential...
Abstract
Ductile iron has far superior mechanical properties compared to gray iron as well as significantly improved castability and attractive cost savings compared to cast steel. This chapter begins with information on graphite morphology and matrix type. It then discusses the advantages and applications of ductile iron. Next, the effects of various factors on the grades, chemistry, matrix, and mechanical properties of ductile iron are covered. This is followed by a section detailing the ductile iron treatment methods and the quality control methods used. Guidelines for gating and feeder design are then provided. Further, the chapter addresses the technology of ductile iron castings, including the performance and geometric attributes, molding and core-making processes used, material grades, mechanical properties, and chemical compositions of a few applications. Finally, it describes ductile iron casting defects and presents practical cases of problem-solving.
Book Chapter
Case Studies of Steel Component Failures in Aerospace Applications
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130351
EISBN: 978-1-62708-284-6
..., inboard flap hinge bolt, nose landing gear piston axle, multiple-leg aircraft-handling sling, aircraft hoist sling, internal spur gear, and MLG axle. In addition, the chapter provides information on full-scale fatigue testing, nondestructive testing, and failure analysis of fin attach bolts. high...
Abstract
This chapter presents various case histories that illustrate a variety of failure mechanisms experienced by the high-strength steel components in aerospace applications. The components covered are catapult holdback bar, AISI 420 stainless steel roll pin, main landing gear (MLG) lever, inboard flap hinge bolt, nose landing gear piston axle, multiple-leg aircraft-handling sling, aircraft hoist sling, internal spur gear, and MLG axle. In addition, the chapter provides information on full-scale fatigue testing, nondestructive testing, and failure analysis of fin attach bolts.
1