Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030005
EISBN: 978-1-62708-282-2
... Abstract This chapter discusses some important factors involved in the atmospheric corrosion of engineering materials. The discussion begins with a description of elements necessary for the operation of a galvanic corrosion cell and corrosion reactions, followed by the types of atmospheric...
Image
Published: 01 March 2001
Fig. 16 Atmospheric corrosion test rack More
Image
Published: 01 January 2000
Fig. 7 Atmospheric-corrosion test rack More
Image
Published: 01 January 2000
Fig. 1 Atmospheric corrosion versus time in a semiindustrial or industrial environment More
Image
Published: 01 October 2011
Fig. 8.13 Atmospheric corrosion versus time of carbon, copper steels, and HSLA weathering steels in a semiindustrial or industrial environment More
Image
Published: 01 December 2001
Fig. 29 Atmospheric corrosion versus time in a semi-industrial or industrial environment. Source: Ref 9 More
Image
Published: 01 January 2000
Fig. 6 Specimens for atmospheric stress-corrosion tests. (a) U-beam specimen. (b) Bent-beam specimen. (c) Direct tension specimen. (d) C-ring specimen More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.t65940451
EISBN: 978-1-62708-302-7
... for Porosity in Gold Coatings on Metal Substrates by Paper Electrography • B 808, Test Method for Monitoring of Atmospheric Corrosion Chambers by Quartz Crystal Microbalances • B 810, Test Method for Calibration of Atmospheric Corrosion Test Chambers by Change in Mass of Copper Coupons • B 825...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310027
EISBN: 978-1-62708-286-0
... Abstract This chapter explores the behavior of stainless steel in media that promote corrosion. The forms of corrosion covered are uniform corrosion, atmospheric corrosion, localized corrosion, pitting corrosion, crevice corrosion, and grain boundary corrosion. The chapter discusses...
Image
Published: 01 November 2007
Fig. 7.26 Corrosion behavior of alloy 800 in the MPC coal gasification atmosphere (0.5% H 2 S at 900 °C or 1650 °F, and 6.9 MPa or 1000 psig) showing oxide scales during the protective stage and oxides/sulfides after breakaway corrosion. Source: Ref 63 More
Image
Published: 01 November 2007
Fig. 7.29 Corrosion of Fe-Cr-Ni alloys in the MPC coal gasification atmosphere with 1.0 and 1.5% H 2 S (see Tables 7.4 and 7.5 for gas composition). Source: Ref 60 More
Image
Published: 01 December 2001
Fig. 6 Stress corrosion of sand-cast AZ91C (T4 and T6) in rural atmosphere. Source: Ref 10 More
Image
Published: 01 December 2001
Fig. 11 Stress corrosion of ZK60A-T5 extrusion in rural atmosphere. Source: Ref 10 More
Image
Published: 01 July 2000
Fig. 7.85 Stress-corrosion behavior of steels exposed to marine atmospheres at 75% of the yield strength. Source: Ref 123 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910193
EISBN: 978-1-62708-250-1
... Abstract Corrosive environments can be broadly classified as atmospheric, underground/soil, water, acidic, alkaline, and combinations of these. Complicating matters is the fact that there are important variables, for example, pH, temperature, and the presence of biological organisms, that can...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870135
EISBN: 978-1-62708-299-0
... Abstract Aluminum products are used extensively in natural atmospheres and in and around water. They are also widely used in building materials and as containers for chemicals and food and beverage products. This chapter discusses the corrosion mechanisms associated with these environments...
Image
Published: 01 January 2000
Fig. 21 Corroded weathering steel formwork on the ceiling of a parking garage. The seams in this corrugated structure act as condensation traps and lead to wet atmospheric corrosion. More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910427
EISBN: 978-1-62708-250-1
... separately in this chapter, the other laboratory tests covered under this category are simulated atmosphere tests, salt-spray tests, and immersion tests. Only corrosion testing in the atmosphere is discussed in the section on field tests. Corrosion monitoring techniques are finally considered, covering...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170193
EISBN: 978-1-62708-297-6
.... high-strength low-alloy steel microalloying Composition Introduction and Overview High-strength low-alloy (HSLA) steels, or microalloyed steels, are designed to provide better mechanical properties and/or greater resistance to atmospheric corrosion than conventional carbon steels...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430147
EISBN: 978-1-62708-253-2
...) Chelate corrosion Fire-side corrosion: Waterwall corrosion or reduced atmosphere corrosion Fuel ash corrosion Coal-ash corrosion Oil-ash corrosion Hot corrosion Acid dew point corrosion or cold-end corrosion SCC Polythionic acid stress-corrosion cracking (PASCC) Fire...