Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060407
EISBN: 978-1-62708-261-7
... ductile than martensitic stainless steels. Examples: 630, 17-4PH, Custom 455, PH 13-8 Mo, ASTM A453-B17B, AISI 660 Nickel-base alloys       Nickel-copper Ultimate tensile strength, 480 to 550 MPa (70 to 80 ksi). Can be cold worked, but not heat treated. Example: Monel       Nickel-copper...