... and some filler metals subject to galvanic corrosion See Tables 3 and 4 for corrosion rates of galvanic couples. Metal Composition, wt% C Mn Si Cr Ni Fe Others Base metals ASTM A53, grade B 0.30 1.20 … … … bal … ASTM A285, grade C 0.22 0.90 … … … bal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930217
EISBN: 978-1-62708-359-1
... properties of the heat-affected zone in a carbon-manganese grade steel, (a) Effect of multiple PWHT at 600 °C (1110 °F). (b) Effect of PWHT time at 600 °C (111 0 °F). (c) Effect of PWHT temperature. Source: Ref 14 Charpy Tests Five testing temperatures were chosen, and three specimens were tested...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820013
EISBN: 978-1-62708-339-3
... corrosion See Tables 6 and 7 for corrosion rates of galvanic couples. Metal Composition, wt% C Mn Si Cr Ni Fe Others Base metals ASTM A53, grade B 0.30 1.20 ... ... ... bal ... ASTM A285, grade C 0.22 0.90 ... ... ... bal ... Filler metals E6010...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930365
EISBN: 978-1-62708-359-1
... for selected thicknesses of structural carbon steels (AWS D1.1) ASTM designations Thickness of thickest part at point of welding ( t ) Minimum temperature (a) (b) (d) mm in. °C °F Category A: Shielded metal arc welding with other than low-hydrogen electrodes A 36 (c) ; A 53, grade B...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090419
EISBN: 978-1-62708-266-2
... associated with this state of SCC. Fig. 18.8 Hydrogen cyanide cracking in a schedule 80 ASTM A53 black pipe steel drain line. (a) Primary crack penetration has advanced toward the outside diameter. 2% nital etch. Original magnification: 50×. (b) The primary crack is intergranular and contains numerous...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030292
EISBN: 978-1-62708-282-2
... 26–28 bal 29.5–32.5 3–4 1.4Cu, 2.5Mn 255 S32550 0.04 24–27 bal 4.5–6.5 2–4 2.5Cu, 1.5Mn, 0.25N 100 (ASTM A351) S32760 0.03 55 bal 6–8 3–5 0.7Cu, 0.25N, 0.7W 2507 S32750 0.03 24–26 bal 6–8 3–5 0.5Cu, 0.24–0.32N 2205 S31803 0.03 21–23 bal 4.5–6.5 2.5–3.5 0.08...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.t69870201
EISBN: 978-1-62708-344-7
... that are determined from finite-element solution or other approximation approaches. Fig. 9.5 Stress-intensity factors for commonly encountered service conditions. Source: Ref 12. (a) Penny-shaped crack in uniform tension in infinite body. (b) Edge crack in a semi-infinite sheet subjected to tension. (c) Single...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.9781627083409
EISBN: 978-1-62708-340-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.9781627083447
EISBN: 978-1-62708-344-7