Published: 01 December 2015
Fig. 13 Section of ASTM A106 carbon steel pipe with wall severely damaged by hydrogen attack. The pipe failed after 15 months of service in hydrogen-rich gas at 34.5 MPa (5000 psig) and 320 °C (610 °F). (a) Overall view of failed pipe section. (b) Microstructure of hydrogen-attacked pipe near More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030089
EISBN: 978-1-62708-282-2
... brine and raw river water and was cathodic to ASTM A285, grade C, in the alkaline-chloride stream. When the base metal was changed to ASTM A53, grade B, and A106, grade B, it was found that E7010-Al weld metal was cathodic to both when exposed to raw brine at 50 °C (120 °F). Finally, routine...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460253
EISBN: 978-1-62708-285-3
... velocity by time-of-flight optical particle diagnostics (cold spray meter); Vickers microhardness; surface roughness by stylus profilometer; surface topography by confocal microscopy; porosity measurement by image analysis; bond strength by ASTM C633 ( Ref 10.16 ) and/or modified ASTM E8; tensile testing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030215
EISBN: 978-1-62708-282-2
... that the material is obtained as ordered and that it meets all the requirements of the application. Perhaps the best known and most widely used specifications are the standards of ASTM International, which presents thousands of specifications for virtually all metal and nonmetal materials of construction...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820013
EISBN: 978-1-62708-339-3
... and was cathodic to ASTM A285, grade C, in the alkaline-chloride stream. When the base metal was changed to ASTM A53, grade B, and A106, grade B, it was found that E7010-Al weld metal was cathodic to both when exposed to raw brine at 50 °C (120 °F). Finally, routine inspection of a column in which a mixture...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930217
EISBN: 978-1-62708-359-1
... also illustrates a method for calculating the length and the percent of the GCHAZ. Evaluation of wide plate tests suggests that fractures are likely to initiate from GCHAZ where the grain size is greater than 80 μm (0.0024 in.), or ASTM No. 4 ( Ref 22 , 23 ). To reduce welding costs, narrow groove...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490001
EISBN: 978-1-62708-340-9
... 1.3. ASTM specifications for steels commonly used in refinery and petrochemical equipment (a) ( Ref 10 ) Material Pipes and tubes Plates Castings Forgings Carbon steel A53,A106,A134,A135,A139,A155,A178,A179,A192,A210,A214,A226,A333,A334,A381,A524,A587 A283,A285,A299,A433,A443,A455...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030292
EISBN: 978-1-62708-282-2
... 26–28 bal 29.5–32.5 3–4 1.4Cu, 2.5Mn 255 S32550 0.04 24–27 bal 4.5–6.5 2–4 2.5Cu, 1.5Mn, 0.25N 100 (ASTM A351) S32760 0.03 55 bal 6–8 3–5 0.7Cu, 0.25N, 0.7W 2507 S32750 0.03 24–26 bal 6–8 3–5 0.5Cu, 0.24–0.32N 2205 S31803 0.03 21–23 bal 4.5–6.5 2.5–3.5 0.08...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930365
EISBN: 978-1-62708-359-1
... for selected thicknesses of structural carbon steels (AWS D1.1) ASTM designations Thickness of thickest part at point of welding ( t ) Minimum temperature (a) (b) (d) mm in. °C °F Category A: Shielded metal arc welding with other than low-hydrogen electrodes A 36 (c) ; A 53, grade B...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.9781627083409
EISBN: 978-1-62708-340-9