... Company of Pittsburgh. This was followed in 1948 by Armco’s development of 17-4 PH and later by 17-7 PH and PH 15-7 Mo. Allegheny Ludlum Steel Company developed A286, AM350, and AM355. The Carpenter Steel Company developed Custom 450, Custom 455, and Custom 630. These alloys contain 11 to 18% chromium, 3...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930179
EISBN: 978-1-62708-359-1
... 15-7 Mo S15700 E308, or E309 AMS 5812C (PH 15-7 Mo) E309 or ER309, E310 or ER310 AM350 S35000 AMS 5775A (AM350) AMS 5774B (AM350) E308 or ER308, E309 or ER309 AM355 S35500 AMS 5781A (AM355) AMS 5780A (AM355) E308 or ER308, E309 or ER309 Source: Ref 2 Semiaustenitic...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900125
EISBN: 978-1-62708-350-8
... and 300 series Martensitic stainless steels of the 400 series such as 422 and 440 Precipitation-hardening stainless steels such as 13-8 PH, 15-5 PH, 17-4 PH, 17-7 PH, A-286, AM350, and AM355 What is the product to be manufactured and how complex is the part geometry? Under what type...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310137
EISBN: 978-1-62708-286-0
... deplete the alloy of carbon and nitrogen, precluding the action of the conditioning heat treatment, which relies on manipulating the amount of carbon in solution. In AM350 and AM355, it is the precipitation of (Cr,Fe) 2 N within the martensite phase that is responsible for age hardening. In addition...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310203
EISBN: 978-1-62708-326-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090095
EISBN: 978-1-62708-266-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.9781627082860
EISBN: 978-1-62708-286-0