1-14 of 14 Search Results for

8822

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130601
EISBN: 978-1-62708-284-6
..., previous treatment rolled Fig. A11.17 1¾ Ni Mo, analysis wt%, austenitized at 845 °C, previous treatment rolled Fig. A11.18 1¼ Ni Cr, analysis wt%, austenitized at 850 °C, previous treatment rolled Fig. A11.19 ½ Ni Cr Mo (8622–8627) (8720) (8822), analysis wt%, austenitized at 830 °C...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250001
EISBN: 978-1-62708-345-4
..., 8625, 8822 Drives Industrial Helical, spur rack and pinion, worm 1045, 1050, 4140, 4142, 4150, 4320, 4340, 4620 Tractor-accessory Crossed-axis helical, helical 1045, 1144, 4118, 4140 Engines Heavy truck Crossed-axis helical, spur, worm 1020, 1117, 4140, 4145, 5140, 8620...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130563
EISBN: 978-1-62708-284-6
... 1.6543 8720 1.6543 8720H 1.6543 8822 1.6543 8822H 1.6545 8630 1.6545 8630H 1.6546 8640 1.6546 8640H 1.6546 8740 1.6546 8740H 1.6562 E4340 1.6562 E4340H 1.6565 4340 1.6565 4340H 1.6755 4718 1.6755 4718H 1.7006 5140H 1.7006 5150 1.7007...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130537
EISBN: 978-1-62708-284-6
...–1525 4820 800–830 1475–1525 8115 845–870 1550–1600 8615 845–870 1550–1600 8617 845–870 1550–1600 8620 845–870 1550–1600 8622 845–870 1550–1600 8625 845–870 1550–1600 8627 845–870 1550–1600 8720 845–870 1550–1600 8822 845–870 1550–1600 9310 790–830...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130541
EISBN: 978-1-62708-284-6
... 12.2 12.8 … … … … 8645 Oil hardened, tempered 11.7 12.2 12.8 … … … … 8650 Oil hardened, tempered 11.7 12.2 12.8 … … … … 8655 Oil hardened, tempered 11.7 12.2 12.8 … … … … 8720 Unknown 11.3 (k) … … … … … 14.6 (l) 8822 Unknown 11.3 12.2 12.9...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130551
EISBN: 978-1-62708-284-6
... 40NiCrMo2KB 7845 40NiCrMo2 7874 40NiCrMo2 … 8822 No international equivalent 9254 No international equivalent 9260 … G4801 SUP7 970 250A58 (En45A) 970 250A61 (En45A) 60S7 61S7 … … E9310 1.6657, 14NiCrMo13 4 … 970 832H13 970 832M13 (En36C) S.157 16NCD13 6932 15NiCrMo13 9335 10NiCrMo13...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250089
EISBN: 978-1-62708-345-4
..., 4320, 4419, 4422, 4615, 4617, 4620, 4621, 4718, 4720, 4815, 4817, 4820, 5015, 5115, 5120, 6118, 8115, 8617, 8620, 8622, 8822, 9310, 94B15, 94B17 125–175 Hot rolled, annealed, or cold drawn 25–13 1–2 2 1.50 0.060 49 160 S4, S2 M2, M7 12–2.5 3–10 1 1.50 0.060 52 170 2–1.5 11–19 1...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440125
EISBN: 978-1-62708-262-4
...–1.00 0.035 0.040 0.15–0.30 0.40–0.70 0.40–0.60 0.15–0.25 8720 G87200 0.18–0.23 0.70–0.90 0.035 0.040 0.15–0.30 0.40–0.70 0.40–0.60 0.20–0.30 8740 G87400 0.38–0.43 0.75–1.00 0.035 0.040 0.15–0.30 0.40–0.70 0.40–0.60 0.20–0.30 8822 G88220 0.20–0.25 0.75–1.00 0.035...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.9781627082846
EISBN: 978-1-62708-284-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250039
EISBN: 978-1-62708-345-4
... 0.70–0.90 ... 0.80–1.10 ... (b) , (c) 8617 0.15–0.20 0.70–0.90 0.40–0.70 0.40–0.60 0.15–0.25 (b) , (c) 8620 0.18–0.23 0.70–0.90 0.40–0.70 0.40–0.60 0.15–0.25 (b) , (c) 8720 0.18–0.23 0.70–0.90 0.40–0.70 0.40–0.60 0.20–0.30 (b) , (c) 8822 0.20–0.25 0.75...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310055
EISBN: 978-1-62708-326-3
... 730 (1345) 765 (1410) 690 (1270) 665 (1230) 250 (485) 8720 G87200 730 (1350) 830 (1530) 770 (1420) 660 (1220) 395 (740) 8740 G87400 730 (1345) 780 (1435) 720 (1330) 660 (1220) 320 (605) 8822 G88220 720 (1330) 840 (1540) 785 (1445) 645 (1195) 385 (725) E9310 G93106...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310095
EISBN: 978-1-62708-326-3
... 0.18–0.23 0.70–0.90 0.15–0.35 0.40–0.70 0.40–0.60 0.20–0.30 8740 G87400 0.38–0.43 0.75–1.00 0.15–0.35 0.40–0.70 0.40–0.60 0.20–0.30 8822 G88220 0.20–0.25 0.75–1.00 0.15–0.35 0.40–0.70 0.40–0.60 0.30–0.40 E9310 G93106 0.08–0.13 0.45–0.65 0.15–0.35 3.00–3.50 1.00–1.40...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310203
EISBN: 978-1-62708-326-3
..., for example, that to obtain 60 HRC in carburized 8822, a quench cooling rate corresponding to 8/16 in. Jominy position is required. With the same steel, a 3% ammonia addition to the carburizing gas reduces this minimum quench cooling rate to 11/16 in. Jominy position. Of even more importance is the ability...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310163
EISBN: 978-1-62708-326-3
... 8620 845–870 1550–1600 8622 845–870 1550–1600 8625 845–870 1550–1600 8627 845–870 1550–1600 8720 845–870 1550–1600 8822 845–870 1550–1600 9310 790–830 1450–1525 Alloy H steels 3310H 845 1550 4027H 870 1600 4028H 870 1600 4032H 870 1600 4815H...