1-12 of 12 Search Results for

60Cu-40Zn

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 August 1999
) and (d) 0.3% C (0.30C-0.005Si-0.85Mn, wt%). Braze welded using a gas torch and a 60Cu-40Zn brass filler metal, (c) Weld region. The dark band in the parent metal adjacent to the weld is an artifact of the etching process, arising because of the electrochemical difference between the copper and iron More
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300163
EISBN: 978-1-62708-323-2
...-40Zn C28000, muntz metal       97Cu-3Si ASTM B97, C65500, silicon brass       60Cu-0.85Sn-39.7Zn ASTM B21, C46400 Bronzes    Phosphor, 94.8Cu-5Sn-0.2P ASTM B139, C51000    Leaded phosphor, 68Cu-4Pb-4Sn-4 Zn ASTM B139, C54400    Aluminum, 90Cu-2Fe-7Al-1Mn C61400    Silicon...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240469
EISBN: 978-1-62708-251-8
... 41 90 13 47 64 HRF Hard 434 63 407 59 5 73 HRB Cartridge brass, 70% C26000 70Cu-30Zn Annealed 359 52 131 19 55 72 HRF Hard 531 77 441 64 8 82 HRB Muntz metal C28000 60Cu-40Zn Annealed 379 55 117 17 45 80 HRF Half-hard 490 71 352 51 15 75 HRB...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170457
EISBN: 978-1-62708-297-6
... is essentially a cast version of the familiar 60Cu-40Zn Muntz metal (C28000). High-Strength Brasses Also called manganese bronzes and high-tensile brasses, these Cu-Zn-Fe-Al-Mn alloys (C86100 to C86800) are among the strongest (as cast) copper-base materials. The mechanical properties of the high-strength...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060333
EISBN: 978-1-62708-261-7
..., 70% C26000 70Cu-30Zn Annealed Hard 357 532 52 77 133 441 19 64 55 8 72 HRF 82 HRB Muntz metal C28000 60Cu-40Zn Annealed Half-hard 378 490 55 71 119 350 17 51 45 15 80 HRF 75 HRB High-lead brass C35300 62Cu-36Zn-2Pb Annealed Hard 350 420 51 61 119 318 17 46 52 7 68 HRF...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350043
EISBN: 978-1-62708-315-7
... 2 Steel, 1032 FOF 0.35 0.25 2 Ti-6Al-4V FOF 0.34 0.29 2 Au Ag IS 0.53 … 1 Au IS 0.49 … 1 Brass, 60Cu-40Zn Steel, tool POR … 0.24 3 Cd Cd IS 0.79 … 1 Fe IS 0.52 … 1 Co Co IS 0.56 … 1 Cr IS 0.41 … 1 Cr Co IS 0.41 … 1 Cr...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060315
EISBN: 978-1-62708-261-7
..., which retain the good corrosion resistance and formability of copper but are considerably stronger than copper. In some cases, the term bronze is used in trade designations for certain specific copper-base alloys that are actually brasses, such as architectural bronzes (57Cu-40Zn-3 Pb) and commercial...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560309
EISBN: 978-1-62708-291-4
... (49.6Ag-15.0Cu-18.1 Zn-17.3Cd) as a filler metal. Nital. 250×. (b) 0.1% C (0.09C-0.005Si-0.43Mn, wt%). Furnace brazed using copper filler metal. Nital. 250×. (c) and (d) 0.3% C (0.30C-0.005Si-0.85Mn, wt%). Braze welded using a gas torch and a 60Cu-40Zn brass filler metal, (c) Weld region. The dark...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310351
EISBN: 978-1-62708-326-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230047
EISBN: 978-1-62708-351-5
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.9781627082976
EISBN: 978-1-62708-297-6