Published: 01 December 2001
Fig. 11 Corrosion rate versus tungsten content for tantalum-tungsten alloys exposed to concentrated H 2 SO 4 at 180 °C (360 °F) and 210 °C (405 °F) More
Image
Published: 01 November 2007
Fig. 12.5 Alloy 625 overlay superheater tubes (on 15Mo3 steel substrate) after 4.5 years of service in a superheater producing 405 °C (760 °F)/42 bar (609 psi) superheated steam, showing no evidence of corrosion or erosion/corrosion. Source: Ref 24 More
Image
Published: 01 August 1999
×. (b) Austenitized at 860 °C, transformed at 500 °C for 0.5 s. B indicates areas of upper bainite; P indicates areas of pearlite. Picral. 2000×. (c) Austenitized at 860 °C, transformed at 500 °C for 2 s. 405 HV. Picral. 250×. (d) Austenitized at 860 °C, transformed at 500 °C for 2 s. B indicates More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130563
EISBN: 978-1-62708-284-6
... XC 38 TS 1038H XC 42 1045 XC 42 1045H XC 42 TS 1045 XC 42 TS 1045H XC 45 1045 XC 45 1045H XC 48 1045 XC 48 1045H XC 60 1064 XC 65 1064 XC 68 1070 XC 90 1086 Z 2 CND 17.12 316L Z 2 CND 19.15 317L Z 6CA13 405 Z 6 CN 18.09 304 Z 6 CND...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410647
EISBN: 978-1-62708-265-5
... 50.4 482 62 223 460 450 425 425 73.3 … 45.3 59.4 83.2 64.3 49.4 471 … 217 450 440 415 415 72.8 … 44.5 58.8 82.8 63.5 48.4 459 59 212 440 430 405 405 72.3 … 43.6 58.2 82.3 62.7 47.4 447 58 205 430 420...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820077
EISBN: 978-1-62708-339-3
..., and niobium to confer particular characteristics. For example, type 405, containing nominally 12% Cr, is made with lower carbon and a small aluminum addition of 0.20% to restrict the formation of austenite at high temperature so that hardening is reduced during welding. In addition, sulfur or selenium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310247
EISBN: 978-1-62708-286-0
... applications Table 1 Ferritic stainless steels for petroleum industry applications UNS Common name S40500 405 S40900 409 S43000 430 S43035 439 S43400 434 S43600 436 S44200 442 S44400 444 (18-2) S44500 … S44600 446 S44626 26-1 Ti, E-Brite S44627 26-1...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930179
EISBN: 978-1-62708-359-1
... 308,309,312 420(l) 2 or 3 420 431 (l) 2 or 3 410 431 (m) 1 308,309,310 Ferritic steels 405 (n) 2 405Cb,430 405,430 (k) 1 308,309,310 430F,430FSe (k) 1 308,309,312 430,430F, 430FSe (o) 2 430 446 2 446 446 (p) 1 308,309,310 (a) 1, as welded; 2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040059
EISBN: 978-1-62708-300-3
... velocity in./s mm/s 3:1.5:0.5 in. (76:38:12.5 mm) Ti-6242 ring Hydraulic 50 0.28 0.33 0.78 19.8 Mechanical 50 0.42 0.044 16 405 Screw 47 0.44 0.024 22 560 3:1.5:0.25 in. (76:38:6.4 mm) Ti-6242 ring Mechanical 30.8 0.42 0.033 15 380 Screw 37.6 0.2 0.019...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000133
EISBN: 978-1-62708-313-3
... 650 81 510 74 495 72 38 19 9 D-979 Bar 1410 204 1295 188 720 104 1005 146 925 134 655 95 15 15 17 Hastelloy C-22 Sheet 800 116 625 91 525 76 405 59 275 40 240 35 57 61 63 Hastelloy G-30 Sheet 690 100 490 71 … … 315 46 170 25 … … 64 75...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310109
EISBN: 978-1-62708-286-0
... listed in Table 1 with their compositions. Ferritic stainless compositions Table 1 Ferritic stainless compositions Alloy Designation C N Cr Ni Mn Si Mo P S Ti Nb Other 405 S40500 0.08 … 11.5–14.5 0.6 1 1 … 0.04 0.03 … … 0.10–0.30 Al 400 AK alloy 0.05...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140211
EISBN: 978-1-62708-335-5
... 60 415 6 ... ... ... ... ... ... ... 75 25 ... 68 470 59 405 6 10.3 71 68 470 59 405 6 300 150 0.5 55 380 52 360 10 ... ... 67 460 59 405 6 10 57 395 52 360 10 ... ... 68 470 60 415 5 100 55 380 50 345 11 ... ... 67 460 59 405 5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030176
EISBN: 978-1-62708-282-2
.... At higher nickel contents are alloys 400 (N04400), R-405 (N04405), and K-500 (N05500), which are used for certain corrosive chemicals, such as hydrofluoric acid, and for seawater. At higher copper contents are the cupronickels, such as 706 (C70600) and 715 (C71500), which are widely used for seawater...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560459
EISBN: 978-1-62708-291-4
... loadBrale indenter diam. ball indenter indenter 660 620 650 611 640 601 630 591 620 582 610 573 600 564 590 554 580 545 570 535 560 525 550 (505) 517 540 (496) 507 530 (488) 497 520 (480) 488 510 (473) 479 500 (465) 471 490 (456) 460 480 (448) 452 470 441 442 460 433 433 450 425 425 440 415 415 430 405 405...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130529
EISBN: 978-1-62708-284-6
... 50.4 482 62 450 425 425 73.3 … 45.3 59.4 83.2 64.3 49.4 471 … 440 415 415 72.8 … 44.5 58.8 82.8 63.5 48.4 459 59 430 405 405 72.3 … 43.6 58.2 82.3 62.7 47.4 447 58 420 397 397 71.8 … 42.7 57.5 81.8 61.9 46.4 435 57 410 388 388 71.4...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310055
EISBN: 978-1-62708-326-3
... 715 (1315) 765 (1410) 705 (1300) 625 (1160) 287 (550) Molybdenum steels 4023/4024 G40230/G40240 730 (1350) 840 (1540) 780 (1440) 670 (1240) 405 (775) 4027/4028 G40270/G40280 725 (1340) 805 (1485) 760 (1400) 670 (1240) 400 (755) 4032 G40320 725 (1340) 815 (1500) 730...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240433
EISBN: 978-1-62708-251-8
... Composition, wt% C Cr Mo Ni N Other 405 0.08 11.5–14.5 … … … 0.10–0.30 Al 406 0.06 12.0–14.0 … 0.5 … 2.75–4.25 Al; 0.6 Ti 409 0.08 10.5–11.75 … 0.5 … Ti = 6 × C min to 0.75 max 409Cb 0.02 12.5 … 0.2 … 0.4 Nb 429 0.12 14.0–16.0 … … … … 430 0.12 16.0...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130285
EISBN: 978-1-62708-284-6
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.tb.atia.t59340165
EISBN: 978-1-62708-427-7
... forging temperature ranges for some typical alloys Alloy Forging temp, °C (°F) 2014 420–460 (785–860) 2025 420–250 (785–840) 2219 425–470 (800–880) 4032 415–460 (780–860) 5083 405–460 (760–860) 6061 430–480 (810–900) 6069 440–490 (825–915) 7010 370...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370059