... CND 17.11 316 Z 6 CNN6 18.10 347 Z 6 CNT 18.10 321 Z 6 CNU 17.04 431 Z 8C17 430 Z 8 CD 17.01 434 Z 10 C 13 410 Z 10 C 14 410 Z 10 CF 17 430F Z 10 CNF 18.09 303 Z 12 C 13 410 Z 12 C 13 M 403 Z 12 CN 17.08 301 Z 12 CNS 25.20 310 Z 12 CNS 25.20 314...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270072
EISBN: 978-1-62708-301-0
... of flight in which the aircraft had made 403 landings. The hub of the wheel had broken. A portion of the failed hub is shown in Fig. CH4.1 . The aircraft was serviced after 100 hours when the ceramic disc and friction plates were changed and taxiing checks were carried out. After the last servicing at 290...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410579
EISBN: 978-1-62708-265-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820115
EISBN: 978-1-62708-339-3
... the relationships among the various standard grades. Chemical compositions of martensitic stainless steels Table 1 Chemical compositions of martensitic stainless steels UNS No. Type/designation Composition (a) , % C Mn Si Cr Ni P S Other Standard (SAE) grades S40300 403 0.15...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060291
EISBN: 978-1-62708-261-7
... Chemical compositions of martensitic stainless steels Table 12.11 Chemical compositions of martensitic stainless steels UNS No. Type/designation Composition(a), % C Mn Si Cr Ni P S Other Standard (AISI) grades S40300 403 0.15 1.00 0.50 11.5–13.0 … 0.04 0.03...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040025
EISBN: 978-1-62708-300-3
...-4V) Fig. 4.11 Flow stress versus strain and strain rate versus strain, for type 403 stainless steel at 1800, 1950, and 2050 °F (980, 1065, and 1120 °C) (tests were conducted in a mechanical press where strain rate was not constant). [ Douglas et al., 1975 ] Fig. 4.12 Flow stress...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490265
EISBN: 978-1-62708-340-9
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170337
EISBN: 978-1-62708-297-6
... RT RT 480 70 … … 3.1 … … 760 1400 403 58 … … 40 … … 870 1600 330 48 … … 53 … … Extrusion + HT/FL RT RT 454 66 … … 0.5 … … 760 1400 405 59 … … 3.0 … … 870 1600 350 51 … … 19 … … P/M extrusion + HT/NL RT RT 510 74 597 87 2.9...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040007
EISBN: 978-1-62708-300-3
...] Niebel B.W. , Draper A.B. , Wysk R.A. , Modern Manufacturing Process Engineering , 1989 , p 403 – 425 . [Schuler Handbook, 1998] Schuler , Metal Forging Handbook , Springer, Goppingen , Germany , 1998 . [SME Handbook, 1989] Tool and Manufacturers Engineering Handbook...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030159
EISBN: 978-1-62708-349-2
... , Amsterdam , 2000 , p 403 – 432 10.1016/B0-08-042993-9/00069-3 2. Hancox N.L. , Thermal Effects on Polymer Matrix Composites: Part 1, Thermal Cycling , Mater. Des. , Vol 19 , 1998 , p 85 – 91 10.1016/S0261-3069(98)00018-1 3. Timmerman J.F. , Tillman M.S. , Hayes B.S...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310233
EISBN: 978-1-62708-326-3
... Martensitic types 403 S40300 0.15 1.00 0.50 11.5–13.0 … 0.04 0.03 … 410 S41000 0.15 1.00 1.00 11.5–13.5 … 0.04 0.03 … 414 S41400 0.15 1.00 1.00 11.5–13.5 1.25–2.50 0.04 0.03 … 416 S41600 0.15 1.25 1.00 12.0–14.0 … 0.06 0.15 min 0.6 Mo (b) 416Se S41623...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140193
EISBN: 978-1-62708-335-5
... treatment, 2 h at 504–521 °C (940–970 °F), 14 h at 529 °C (985 °F), water quench, 24 h at room temperature, plus 5 h at 188 °C (370 °F), air cooled. Average mechanical properties for permanent mold castings: ultimate tensile strength, 439 MPa (63.7 ksi); tensile yield strength, 403 MPa (58.5 ksi). Average...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050175
EISBN: 978-1-62708-311-9
... initiated from rolling seam. (i) SAE type 403 stainless steel as quenched and tempered; microstructure is predominantly tempered martensite with cracking promoted by the seam. Vilella’s reagent. 100×. (j) SAE 4118 carburized steel as quenched and tempered; microstructure is tempered martensite with quench...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550299
EISBN: 978-1-62708-307-2
... 331 48 413 60 2.3 20–30 18–27 760 1400 310 45 430 62 … … … Extrusion + HT/duplex RT RT 480 70 … 3.1 … … 760 1400 403 58 … … 40 … … 870 1600 330 48 … … 53 … … Extrusion + HT/FL RT RT 454 66 … … 0.5 … … 760 1400 405 59 … … 3.0...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240433
EISBN: 978-1-62708-251-8
... properties are given in Table 23.4 . Composition of select martensitic stainless steels Table 23.3 Composition of select martensitic stainless steels Type Composition, wt% C Mn Si Cr Ni P S Other 403 0.15 1.00 0.50 11.5–13.0 … 0.04 0.03 … 410 0.15 1.00 1.00 11.5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120295
EISBN: 978-1-62708-269-3
... industries Elgiloy Specialty Metals 11777 Bee St. Dallas, TX 75234 Tel: 888-403-2091 Fax: 972-247-2243 Source for high-quality alloys Ellett Industries, Ltd. 1575 Kingsway Ave. Port Coquitlam BC V3C4E5 Canada Tel: 604-941-8211 Fax: 604-941-7669 Worldwide designers and fabricators of heat...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540397
EISBN: 978-1-62708-309-6
...) 6061–T651 289 41.9 Bend T-L 29.1 26.5 41.6 37.9 … … … … 7039–T6 381 55.3 Bend T-L 32.3 29.4 33.5 30.5 … … … … 7075–T651 536 77.7 Bend T-L 22.5 20.5 27.6 25.1 … … … … 7075–T7351 403 58.5 Bend T-L 35.9 32.7 32.1 29.2 … … … … 7075–T7351 392...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090341
EISBN: 978-1-62708-266-2
.... , Vol 59 , 1976 , p 403 10.6028/NBS.IR.75-952 14.18 Evans A.G. and Wiederhorn S.M. , Proof Testing of Ceramic Materials—An Analytical Basis for Failure Prediction , Int. J. Fract. Mech. , Vol 10 , 1974 , p 379 10.1007/BF00035499 14.19 Freiman S.W. , Baker T.L...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310123
EISBN: 978-1-62708-286-0
... C Mn S Si Cr Mo Ni Other Other 403 S40300 Wrought 0.15 max 1 0.03 0.5 11.5-13.5 … … … … 410 S41000 Wrought 0.15 max 1 0.03 1 11.5-13.5 … … … … 410S S41003 Wrought 0.03 1 0.03 … 10.5-12.5 … 1.5 0.03 N … 410 S41008 Wrought 0.08 1.5 0.03 1...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500301
EISBN: 978-1-62708-317-1
... Galanulis K. , Optical Measuring Technologies in Sheet Metal Processing , Fourth International Conference and Exhibition on Design and Production of Machines and Dies/Molds , 2007 , p 403 – 411 15.25 3R Technics , http://www.3r-technics.com 15.26 Altan T. , Dissecting Defects...