1-20 of 29 Search Results for

20Cb

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 July 2000
Fig. 7.22 Correlation between the critical pitting temperature and critical pitting potential of 17 high-performance alloys. The alloys are: (1) 317LM, (2) 3RE60, (3) AF22, (4) 44LN, (5) FERRALIUM ALLOY 255, (6) 20CB-3 Alloy, (7) URANUS 86, (8) 2545LX, (9) JESSOP 700, (10) JESSOP 777, (11 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080443
EISBN: 978-1-62708-304-1
..., RA330HC, RA333, RA85H Rolled Alloys 253MA, 254SMO, 44LN Outokumpu 214, 230, 556 Haynes International, Inc. 800HT Special Metals Corporation 20Cb-3, 7-Mo PLUS, 20Mo-4, 20Mo-6, Carpenter Technology Corporation 625 PLUS Duraloy Technologies, Inc. 22-H, MO-RE, Super 22H,TMA AK Steel Corporation PH15-7Mo, PH13...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030176
EISBN: 978-1-62708-282-2
... used in the chemical industry for sulfuric acid service are the copper-containing stainless steels and higher alloys, such as alloy 904L (N08904), 20Cb-3 (N08020), alloy 825 (N08825), and the cast stainless steel CN-7M (J95150), whereas higher-silicon stainless steel, such as S32615, has been used...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910193
EISBN: 978-1-62708-250-1
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820099
EISBN: 978-1-62708-339-3
... of mechanical properties of commonly used stainless steels in the annealed condition UNS No. Common designation Tensile strength Yield strength (a) Elongation, % Hardness (max), HRB MPa ksi MPa ksi Austenitic grades S30400 Type 304 515 75 205 30 40 88 N08020 20Cb-3 585 85...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2010
DOI: 10.31399/asm.tb.hss.t52790241
EISBN: 978-1-62708-356-0
... alloys that contain less than 50% iron and high nickel contents. The UNS designation for alloy 20Cb-3 is N08020. For steel casting alloys in the UNS system, a J xxxxx series of numbers was established. This “J” series is based on the total alloy content. For stainless steel casting alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310247
EISBN: 978-1-62708-286-0
... … J93000 CG-8M … J93254 CK3MCuN … J93402 CH-20 … J94652 CN-3MN … N06022 AL 22 … N08007 CN-7M … N08020 20Cb-3 28 N08020 AL 20 28 N08024 20Mo-4 38 N08026 20Mo-6 … N08028 Sanicro 28 39 N08031 Nicrofer 3127 hMo 54 N08320 20Mod 38 N08366 AL-6X...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820043
EISBN: 978-1-62708-339-3
...–1.75Mo; 0.1–0.35Ti; 1.0–1.75W; 0.25–0.60Nb S70003 Nicrofer 2509 Si7 0.02 2.00 6.5–8.0 8.0–11.0 22.0–25.0 0.025 0.01 0.50Mo; 0.50A1 N08020 20Cb-3 0.07 2.00 1.00 19.0–21.0 32.0–38.0 0.045 0.035 2.0–3.0Mo; 3.0–4.0Cu; 8 × %C min to 1.00 max Nb N08024 20Mo-4 0.03 1.00 0.50 22.5...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310269
EISBN: 978-1-62708-286-0
... 1.0–1.5 … 0.70–1.25 0.045 0.030 … … 23-8N S63018 0.28–0.38 0.28–0.38 22.0–24.0 7.9–9.0 1.5–3.5 … 0.69–0.90 0.045 0.030 … … 19-9DL S63198 0.28–0.36 … 18.0–21.0 8.0–11.0 0.75–1.50 1.0–1.75 0.03–0.80 … … 0.1–0.35 Ti 0.25–0.60 Nb 20Cb-3 N08020 0.07 … 19.0–21.0...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310161
EISBN: 978-1-62708-286-0
...–2150 1900 min … … Stabilized alloys … … … 1000–1600 540–870 321 955–1065 1750–1950 1900 min … … 347, 348 980–1025 1800–1950 1900 min … … 20Cb-3 925–955 1700–1750 … 925–1010 … Moderately alloyed, Cr eq <26 S31725, N08028, JS700 1120–1175 2050–2150 Various...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170257
EISBN: 978-1-62708-297-6
...% Fe. The high-alloy stainless steels were developed for applications where corrosive conditions are too severe for the standard or modified 300-series austenitic grades. A good example of a high-alloy stainless steel is 20Cb-3 (N08020), which was designed for improved resistance to sulfuric acid...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820203
EISBN: 978-1-62708-339-3
... acid (A 262-A) ... (a) Ferric sulfate (A 262-B) 120 0.1 (4) S32100 Type 321 1 h at 675 °C (1250 °F) Nitric acid (A 262-C) 240 0.05 (2) S34700 Type 347 1 h at 675 °C (1250 °F) Nitric acid (A 262-C) 240 0.05 (2) N08020 20Cb-3 1 h at 675 °C (1250 °F) Ferric sulfate (G 28...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080445
EISBN: 978-1-62708-304-1
... … 0.4 19 35 … Bal … … Si: 1.2 AC66 N33228 0.05 28 32 … Bal … … Nb: 0.8, Ce: 0.07 SANICRO 28 N08028 0.01 27 31 … Bal 3.5 … Cu: 1.0 20Cb-3 N08020 0.02 20 33 … Bal 2.2 … Cu: 3.3, Cb: 0.5 20Mo-4 N08024 0.02 23.5 37 … Bal 3.8 … Cu: 1.0, Cb: 0.25 20Mo...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310233
EISBN: 978-1-62708-326-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030215
EISBN: 978-1-62708-282-2
... with tantalum, is used in types 309Cb, 310Cb, and 347 austenitic stainless steels at a minimum combined concentration of approximately ten times the carbon content. The higher-nickel alloys 20Cb-3, alloy 625, and alloy G contain even higher concentrations of niobium—up to a maximum of approximately 4...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030096
EISBN: 978-1-62708-282-2
... … 1.4439 18 14 4.3 0.13 Nitronic 50 21 14 2.2 0.20 20Cb-3 20 33 2.4 … Alloy 904L 20 25 4.2 … 2RK65 20 25 4.5 … JS700 21 25 4.5 … 19/25LC 20 25 4.8 … AL-6X 20 24 6.6 … 254SMO 20 18 6.1 0.20 19/25HMO 21 25 5.9 0.15 Filler metals Type...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060291
EISBN: 978-1-62708-261-7
...%), the UNS designation consists of the letter “N” followed by a five-digit number. Examples include N08020 (20Cb-3), N08024 (20Mo-4), N08026 (20Mo-6), N08366 (AL-6X), and N08367 (AL-6XN). Cast Stainless Steel Designations For cast stainless steels, the High Alloy Product Group of the Steel Founders...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080201
EISBN: 978-1-62708-304-1
... °F). Review of the test data generated at 650 °C (1200 °F) for 10,000 h in the MPC test programs summarized in Howes’s report ( Ref 60 ) showed that alloys containing at least 18% Cr, which included 304, 309, 310, 312, 329, 22-13-5, 29-4-2, Ebrite 26-1, 446, 20Cb-3, 800, 253MA, Crump 25, 825, RA333...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090095
EISBN: 978-1-62708-266-2