Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310137
EISBN: 978-1-62708-286-0
... as opposed to the higher carbon found in the martensitic stainless steels. The early alloys of this type, 177 PH and 17-4 PH, contained up to 10% δ-ferrite stringers, which caused poor through-thickness toughness. This would be expected from the Schaeffler-Delong diagram, but this is asking too much...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2010
DOI: 10.31399/asm.tb.hss.t52790185
EISBN: 978-1-62708-356-0
... and later by 17-7 PH and PH 15-7 Mo. Allegheny Ludlum Steel Company developed A286, AM350, and AM355. The Carpenter Steel Company developed Custom 450, Custom 455, and Custom 630. These alloys contain 11 to 18% chromium, 3 to 27% nickel, and smaller amounts of additional metals, including aluminum, copper...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310233
EISBN: 978-1-62708-326-3
... Cu; 0.15–0.45 Nb 17-7 PH S17700 0.09 1.00 1.00 16.0–18.0 6.5–7.75 0.04 0.04 0.75–1.5 Al (a) Single values are maximum values unless otherwise indicated. (b) Optional For cast stainless steels, the High Alloy Product Group of the Steel Founders’ Society of America...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140133
EISBN: 978-1-62708-264-8
.... , Handbook of Stainless Steels , McGraw-Hill Book Co. , New York , 1977 13.6. Nehrenberg A.E. and Lillys P. , High Temperature Transformations in Ferritic Stainless Steels Containing 17 to 25% Chromium , Trans. ASM , Vol 46 , 1954 , p 1177 – 1213 . 13.7. Heat Treater’s Guide...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900125
EISBN: 978-1-62708-350-8
... stainless steels such as 13-8 PH, 15-5 PH, 17-4 PH, 17-7 PH, A-286, AM350, and AM355 Table 1 lists the compositions of some typical nitridable steels. Compositions of selected nitridable steels Table 1 Compositions of selected nitridable steels Alloy steels (a) Composition, % C Cr...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440175
EISBN: 978-1-62708-262-4
...–14.5 6.25–7.0 0.50 0.30 0.55–0.9 … … … … Semiaustenitic grades S17700 631 17-7 PH 0.09 16.0–18.0 6.5–7.75 1.0 1.0 … 0.75–1.5 … … … S15700 632 PH 15-7 Mo 0.09 14.0–16.0 6.5–7.25 1.0 1.0 … 0.75–1.5 2.0–3.0 … … S35000 633 AM-350 0.07–0.11 16.0–17.0 4.0...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310247
EISBN: 978-1-62708-286-0
...” Precipitation hardening stainless steels for petroleum industry applications Table 3 Precipitation hardening stainless steels for petroleum industry applications UNS Common name Hardness, HRC, max (a) S13800 13-8 PH … S15500 15-5 PH 33 S15700 15-7 PH 32 S17400 17-4 PH 33...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000005
EISBN: 978-1-62708-312-6
.... The precipitate formed is a copper-rich fcc phase. In the case of a semiaustenitic PH alloy, such as 17-7 PH, the M s temperature is lower than room temperature. In the solution-annealed condition, the matrix is fully austenitic, exhibiting good ductility. After forming, a conditioning heat treatment...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310269
EISBN: 978-1-62708-286-0
... 17-7 PH S17700 0.09 … 16.0–18.0 6.5–7.75 1.00 … 1.00 0.040 0.030 … Al 0.75–1.5 15-7 PH S15700 0.09 … 14.0–16.0 6.5–7.75 1.00 2.0–3.0 1.00 0.040 0.030 … Al 0.75–1.5 AM-350 S35000 0.07–0.11 0.07–0.13 16.0–17.0 4.0–5.0 0.50–1.25 2.5–3.25 0.50 0.040 0.030...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170257
EISBN: 978-1-62708-297-6
... … 0.10–0.50 Nb, 1.5–2.5 Cu S13800 … PH 13-8 Mo (XM-13) 0.05 12.25–13.25 7.5–8.5 0.20 0.10 … 0.90–1.35 Al 2.0–2.5 0.01 … S36200 … Almar 362 (XM-9) 0.05 14.0–14.5 6.25–7.0 0.50 0.30 0.55–0.9 … … … … Semiaustenitic grades S17700 631 17-7 PH 0.09 16.0–18.0 6.5–7.75...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310173
EISBN: 978-1-62708-286-0
... diagram to avoid mixtures of ferrite and austenite since the great difference in their great strengths can cause failures. Duplex stainless steels and other alloys (e.g., 17-7 PH) that have high levels of ferrite in austenite or austenite in ferrite at the hot-working temperature exhibit reduced hot...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.9781627082860
EISBN: 978-1-62708-286-0
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350095
EISBN: 978-1-62708-315-7
... series Austenitic stainless steels: 200 and 300 series Precipitation-hardened stainless steels: 13-8 PH, 15-5 PH, 17-4 PH, 17-7 PH, A-286, AM 350 ( Ref 14 ), and AM 355 Fig. 7 Factors affecting the microhardness profile of a nitrided steel. The hardness of the compound zone is unaffected...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090095
EISBN: 978-1-62708-266-2
..., Institute of Civil Engineers, July 1971 10.1680/eoeompins.44579.0013 4.50 Cochran R.W. and Staehle R.W. , Corrosion , Vol 11 , 1968 , p 369 10.5006/0010-9312-24.11.369 4.51 Money K.L. and Kirk W.W. , Mater. Perform. , Vol 17 ( No. 7 ), July 1978 , p 28...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060291
EISBN: 978-1-62708-261-7
... S17700 631 17-7 PH 0.09 16.0–18.0 6.5–7.75 1.0 1.0 … 0.75–1.5 … … … S15700 632 PH 15-7 Mo 0.09 14.0–16.0 6.5–7.25 1.0 1.0 … 0.75–1.5 2.0–3.0 … … S35000 633 AM-350 0.07–0.11 16.0–17.0 4.0–5.0 0.50–1.25 0.50 … … 2.5–3.25 0.07–0.13 … S35500 634 AM-355 0.10...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.9781627083126
EISBN: 978-1-62708-312-6
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410579
EISBN: 978-1-62708-265-5
.... , Ferrite in Austenitic Stainless Steel Weld Metal , Weld. J. , Vol 53 ( No. 7 ), 1974 , p 273s – 286s 23.9 Fischer G.J. and Maciag R.J. , The Wrought Stainless Steels , Handbook of Stainless Steels , McGraw-Hill , p 1–1 to 1–10 23.10 Stainless Steels, in Metals Handbook...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290201
EISBN: 978-1-62708-319-5
... As-sintered Heat treated As-sintered Heat treated MPa ksi MPa ksi Hydrogen 28 40 820 119 1085 157 7 4 Vacuum 22 39 810 117 1135 165 8 7 Dissociated ammonia 27 40 1000 145 1265 183 3 9 Mechanical property changes for sintered 17-4 PH stainless steel and gain...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030338
EISBN: 978-1-62708-282-2
...-corrosion cracks on external surface of high-pressure gas transmission pipeline. The high-pH form of SCC is intergranular ( Ref 14 ), the cracks propagate between the grains in the metal, and there is usually little evidence of general corrosion associated with the cracking ( Fig. 7 ). The near...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870025
EISBN: 978-1-62708-299-0
.... Specimens were 1.6 × 13 × 75 mm (0.06 × 0.5 × 3.0 in.). The pH values of solutions were adjusted with HCl and NaOH. Test temperature was 60 °C (140 °F). Fig. 7 Corrosion of 99.5% pure aluminum in an aggressive solution. Iron-or silicon-containing impurities present at the surface create local...