Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050343
EISBN: 978-1-62708-311-9
... Fig. A5.1 Tempering curve for 1045 steel. Tempered 1 h at heat; as quenched, 60 HRC at 120 °C (250 °F). Source: Ref 1 Fig. A5.2 Tempering curve for 1144 steel. Tempered 1 h at heat; as quenched, 60 HRC at 120 °C (250 °F). Source: Ref 1 Fig. A5.3 Tempering curve for 4140...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440097
EISBN: 978-1-62708-262-4
...–1.65 0.040 0.08–0.13 1144 G11440 0.40–0.48 1.35–1.65 0.040 0.24–0.33 1146 G11460 0.42–0.49 0.70–1.00 0.040 0.08–0.13 1151 G11510 0.48–0.55 0.70–1.00 0.040 0.08–0.13 Source: Ref 1 Compositions of standard rephosphorized and resulfurized carbon steels Table 6...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140055
EISBN: 978-1-62708-264-8
... 1.45 0.11 S 1144 0.44 1.45 0.26 S Plain carbon manganese steels 1340 0.40 1.75 … 1518 0.18 1.25 … 1541 0.41 1.45 … All steels contain a low level of impurity elements that result from the steelmaking process. These impurity elements can be eliminated from...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130255
EISBN: 978-1-62708-284-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050175
EISBN: 978-1-62708-311-9
.... 9.14 (Part 2) Micrographs of cracks. (e) SAE 4140 steel as quenched and tempered; microstructure is tempered martensite with quench cracking promoted by nonmetallic inclusions. Unetched. 100×. (f) SAE 1144 steel as quenched and tempered; microstructure is tempered martensite where cracking is aided...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130537
EISBN: 978-1-62708-284-6
...–1500 (b) Free-cutting carbon steels 1137 830–855 1525–1575 1138 815–845 1500–1550 1140 815–845 1500–1550 1141 800–845 1475–1550 1144 800–845 1475–1550 1145 800–845 1475–1550 1146 800–845 1475–1550 1151 800–845 1475–1550 1536 815–845 1500–1550 1541...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140039
EISBN: 978-1-62708-264-8
... of banded 1045 steel. Original magnification: 230× Figure 5.6 presents results from a similar test on a ferrite-pearlite banded 1144 steel, using the Knoop indenter. (Like a 1044 steel, 1144 contains 0.44% C, but it also contains elevated sulfur levels, and, as a result, contains significant...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130563
EISBN: 978-1-62708-284-6
... A29 1119 A29 1132 A29 1137 A29 1141 A29 1144 A29 1211 A29 1212 A29 1213 A29 12L13 A29 12L14 A29 1215 A29 1547 A29 1548 A29 15B48H A29 9260 A36 A57 1064 A59 9260 A107 1117 A107 1118 A107 1141 A108 1008 A108 1010...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050215
EISBN: 978-1-62708-311-9
... 0.37/0.44 50/60 Water Water No 1045 0.43/0.50 54/64 Water/P Water/P Yes 1050 0.48/0.55 55/65 Water/P Water/P Yes 1141 0.37/0.45 48/56 Water/P Water/P No 1144 0.40/0.48 55/62 Water/P Water/P Yes 1541 0.36/0.44 53/60 Water/P Water/P No Stress proof 0.36...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310095
EISBN: 978-1-62708-326-3
...–1.65 0.040 0.08–0.13 1144 G11440 0.40–0.48 1.35–1.65 0.040 0.24–0.33 1146 G11460 0.42–0.49 0.70–1.00 0.040 0.08–0.13 1151 G11510 0.48–0.55 0.70–1.00 0.040 0.08–0.13 Compositions of standard rephosphorized and resulfurized carbon steels Table 8 Compositions...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310203
EISBN: 978-1-62708-326-3
... 0.5 48 HRC 43 HRC 42 HRC 25 1 34 HRC 28 HRC 23 HRC 50 2 28 HRC 22 HRC 18 HRC 100 4 21 HRC 18 HRC 16 HRC 1141 oil quenched 13 0.5 52 HRC 49 HRC 46 HRC 25 1 48 HRC 43 HRC 38 HRC 50 2 36 HRC 28 HRC 22 HRC 100 4 27 HRC 22 HRC 18 HRC 1144 oil...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350087
EISBN: 978-1-62708-315-7
... hardening Material Typical hardness, HRC, as affected by quenchant Air (a) Oil (b) Water (b) Plain-carbon steels 1025–1035 … … 33–50 1040–1050 … 52–58 55–60 1055–1075 50–60 58–62 60–63 1080–1095 55–62 58–62 62–65 1125–1137 … … 45–55 1138–1144 45–55 52...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.9781627083119
EISBN: 978-1-62708-311-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130551
EISBN: 978-1-62708-284-6
... 216M36 (En15AM) 970 225M36 35MF4 A35-562 35MF6 … 1957 1140 No international equivalents 1141 … G4804 SUM42 970 212A42 (En8DM) 970 216A42 A35-562 45MF4 … … 1144 1.0727, 45S20 G4804 SUM43 970 212A42 (En8DM) 970 212M44 970 216M44 970 225M44 970 226M44 A35-562 45MF6 4838 CF44SMn28...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050155
EISBN: 978-1-62708-311-9
... 58 57 52 47 43 42 41 40 33 1137 0.40 44 42 40 37 33 30 27 21 91 (a) Normalized at 900 °C (1650 °F); water quenched from 830 to 855 °C (1525 to 1575 °F); average dew point, 13 °C (55 °F) 1141 0.40 49 46 43 41 38 34 28 23 94 (a) 1144 0.40 55 50 47 45 39 32...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050093
EISBN: 978-1-62708-311-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050245
EISBN: 978-1-62708-311-9
... 1144 will have particle buildups around the surface sulfide inclusions. Nonrelevant indications are caused by flux leakage that has no relation to a discontinuity that is considered to be a defect. When it is necessary to recheck lots of parts in which a defect has been found, the parts should be held...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130541
EISBN: 978-1-62708-284-6
... (f) … … … … … … 1137 Unknown 12.8 … … … … … … 1139 Unknown 12.6 (f) … … … … … … 1140 Unknown 12.6 (f) … … … … … … 1141 Unknown … 12.6 (b) … … … … … 1144 Unknown 13.3 … … … … … … 1145 Annealed 11.2 (b) 12.1 (b) 13.0 (b) 13.6...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310163
EISBN: 978-1-62708-326-3
... tempering temperature and “as-quenched” hardness for several steels for both induction hardening and furnace quenched parts Temperature 4140 and 4150 steel Temperature 1141, 1144, or 1045 steel Furnace treat—as quench, HRC Induction harden, HRC Furnace treat—as quench, HRC Induction harden...