Published: 01 March 2002
Fig. 3.31 Microstructure of an improperly carbonitrided AISI/SAE 1117 steel shaft showing various layers below the treated surface. The layers “A” through “E” are shown at higher magnification in Fig. 3.32 . 2% nital and 4% picral etch. 40× More
Image
Published: 01 March 2002
Fig. 3.32 (Part 1) Magnified view of the various layers in the carbonitrided AISI/SAE 1117 steel shaft in Fig. 3.31 . (a) Outer layer of retained austenite and plate martensite (needlelike constituent), (b) a layer of plate martensite and some retained austenite, (c) a layer of fine lath More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130537
EISBN: 978-1-62708-284-6
... 1522 760–790 1400–1450 1524 760–790 1400–1450 1525 760–790 1400–1450 1526 760–790 1400–1450 1527 760–790 1400–1450 Free-cutting carbon steels 1109 760–790 1400–1450 1115 760–790 1400–1450 1117 760–790 1400–1450 1118 760–790 1400–1450 Alloy steels...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250245
EISBN: 978-1-62708-345-4
... cases, and medium-carbon or high-carbon steels are involved. Whether or not the core has a martensitic structure is also a contributing factor in case-depth measurements. Gear steels commonly carbonitrided include carbon steels (1018, 1022, 1117) and alloy steels in the 4100, 4300, 5100, and 8600...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130563
EISBN: 978-1-62708-284-6
... A29 1119 A29 1132 A29 1137 A29 1141 A29 1144 A29 1211 A29 1212 A29 1213 A29 12L13 A29 12L14 A29 1215 A29 1547 A29 1548 A29 15B48H A29 9260 A36 A57 1064 A59 9260 A107 1117 A107 1118 A107 1141 A108 1008 A108 1010...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130541
EISBN: 978-1-62708-284-6
... 11.1 (b) … … 13.1 (b) … … … 1095 Unknown … … … … … … 14.6 (d) 1095 Annealed 11.4 … … … … … … 1095 Hardened 13.0 (b) … … … … … … 1117 Unknown 12.2 (f) … … 13.1 (g) … … … 1118 Unknown 12.2 (f) … … 13.3 (g) … … … 1132 Unknown 12.6...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250001
EISBN: 978-1-62708-345-4
... helical, helical 1045, 1144, 4118, 4140 Engines Heavy truck Crossed-axis helical, spur, worm 1020, 1117, 4140, 4145, 5140, 8620 Equipment Earth moving Spiral/straight bevel, zerol 1045, 4140, 4150, 4340, 4620, 4820, 8620, 9310 Farming Face, internal, spiral/straight bevel, spur...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480095
EISBN: 978-1-62708-318-8
...-2.5Sn 760 1400 876 127 1117 162 1.70 650 1200 979 142 1324 192 2.34 538 1000 1007 146 1386 201 2.63 Ti-4A1 760 1400 669 97 1014 147 4.30 650 1200 731 106 1214 176 7.98 538 1000 772 112 1324 192 9.85 Ti-6Al-4V 460 1400 910 132 1117 162 1.43...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120095
EISBN: 978-1-62708-269-3
...), ~vol% phases MPa ksi MPa ksi 955 °C (1751 °F) furnace cooled 834 121 937 136 19 46 90% alpha; 10% beta 955 °C (1751 °F) water quenched 951 138 1117 162 17 60 50% primary alpha; 50% alpha prime + alpha double prime + retained beta 900 °C (1652 °F) furnace cooled 855 124...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.9781627082846
EISBN: 978-1-62708-284-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.t60400049
EISBN: 978-1-62708-258-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130551
EISBN: 978-1-62708-284-6
... states (SAE) Fed. R. of Germany (DIN) Japan (JIS) United Kingdom (BS) France (AFNOR NF) Italy (UNI) Sweden (SS14) 1108 1.0700, U7S10 1.0702, U10S10 G4804 SUM12 … A35-562 10F1 … … 1110 1.0703, R10S10 G4804 SUM11 … … … … 1117 … G4804 SUM31 970 210A15 970 210M17 (En32M) 970...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310203
EISBN: 978-1-62708-326-3
... 45 HRC 42 HRC 39 HRC 50 2 43 HRC 40 HRC 37 HRC 100 4 39 HRC 37 HRC 32 HRC 1095 oil quenched 13 0.5 60 HRC 44 HRC 41 HRC 25 1 46 HRC 42 HRC 40 HRC 50 2 43 HRC 40 HRC 37 HRC 100 4 40 HRC 37 HRC 30 HRC 1117 water quenched 13 0.5 42 HRC...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250089
EISBN: 978-1-62708-345-4
... (a) Cutter pitch line speed High-speed steel tool material Module Diametral pitch mm in. m/min sfm ISO AISI Wrought free-machining carbon steels Low-carbon resulfurized 1116, 1117, 1118, 1119, 1211, 1212 100–150 Hot rolled or annealed 25–6 1–4 0.3 0.012 185 610 S4, S2 M2, M7...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780204
EISBN: 978-1-62708-281-5
....19680240209 25. Sternstein S.S. and Ongchin L. , Polym. Prepr. , Vol 10 ( No. 2 ), 1969 , p 1117 26. Kambour R.P. , Polymer , Vol 5 , 1964 , p 143 10.1016/0032-3861(64)90128-4 27. Marshall G.P. , Culver L.E. , and Williams J.G. , Proc. R. Soc...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250039
EISBN: 978-1-62708-345-4
...) 1022 0.18–0.23 0.70–1.00 ... ... ... (a) , (b) 1025 0.22–0.28 0.30–0.60 ... ... ... (a) , (b) 1524 0.19–0.25 1.35–1.65 ... ... ... (a) , (b) 1527 0.22–0.29 1.20–1.50 ... ... ... (a) , (b) Resulfurized steels 1117 0.14–0.20 1.00–1.30...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140039
EISBN: 978-1-62708-264-8
... 72.0 … 1386 201 42 412 390 71.5 … 1338 194 41 402 381 70.9 … 1296 188 40 392 371 70.4 … 1248 181 39 382 362 69.9 … 1213 176 38 372 353 69.4 … 1179 171 37 363 344 68.9 … 1158 168 36 354 336 68.4 (109.0) 1117 162 35 345 327 67.9...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410373
EISBN: 978-1-62708-265-5
... 1165 169 13.7 45.0 363 25.4 1 1207 175 1145 166 14.2 45.9 352 50.8 2 1172 170 1103 160 16.0 54.8 341 101.6 4 1138 165 1000 145 15.5 53.4 331 Oil quenched from 800 °C (1475 °F), tempered at 593 °C (1110 °F) 12.7 ½ 1145 166 1117 162 17.1 57.0 331...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.t60400297
EISBN: 978-1-62708-258-7
... apply. For rods, the following ranges and limits for silicon are commonly used; up to SAE 1110 inclusive, 0.10% max; SAE 1117 and over, 0.10% max, 0.10 0.20%, or 0.15 0.35%. Free-machining (rephosphorized and resulfurized) carbon steel compositions (a) When lead ranges or limits are required, the values...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480225
EISBN: 978-1-62708-318-8
... 161 1176 171 5.7 7.8 24 6.65–7.18 380–410 1145 166 1207 175 5.7 5.5 28 1117 162 1169 170 4.0 7.0 22 (a) Radius ( R ) of bend over thickness ( T ) of a side-notched specimen bent slowly around a mandrel Fig. 10.27 Microstructure of properly processed Ti-13V...