Image
Published: 01 August 2018
Fig. 7.26 Cross section of AISI 1015 wire rod, normalized. Ferrite and pearlite (approx. volume fraction 15%). Ferritic grain size ASTM 9 (according to ASTM E112, Ref 16 ). Etchant: nital 2%. Courtesy of ArcelorMittal Aços Longos, Juiz de Fora, MG, Brazil. More
Image
Published: 01 March 2002
Fig. 3.41 Microstructure of an AISI/SAE 1015 casting showing iron sulfide surrounding a manganese sulfide inclusion. Unetched. 2000× More
Image
Published: 01 January 2015
Fig. 8.17 Comparison of austenitic grain size in (a) coarse-grained SAE 1015 steel and (b) fine-grained SAE 4615 steel after carburizing. Light micrographs. Original magnification: 1000×. Source: Ref 8.16 More
Image
Published: 01 December 1999
Fig. 5.6 Prior austenite grain boundaries. (a) Coarse-grained SAE 1015 carbon steel, carburized. 100×. (b) Fine-grained SAE 4615 nickel-molybdenum steel, carburized. 100× More
Image
Published: 31 December 2020
Fig. 20 Effect of normalizing on resistance welded 1015 steel tube. (a) Transverse section with vertical band of the fusion zone and heat affected zone on each side. (b) Normalized tube wit weld zone at center. Light areas are ferrite, dark pearlite. More
Image
Published: 01 December 2003
Fig. 5 The metallographic appearance of AISI 1015 (UNS G10150) steel after a 2 h vacuum nitrocarburizing treatment in an ammonia/methane mixture with 1% oxygen addition More
Image
Published: 01 December 1999
Fig. 1.4 Depth of the oxidized zones vs. carburizing time at different carburizing temperatures for SAE 1015. Source: Ref 6 More
Image
Published: 01 January 2015
Fig. 5.25 Effect of annealing temperature on grain size of Ti-5Al-2.5Sn. Grain growth is very rapid at the beta transus temperature (1015 °C, or 1860 °F) and higher. More
Image
Published: 01 October 2011
Fig. 8.3 Spark patterns used to identify low-, medium-, and high-carbon steels. (a) Sparks from 1015 steel (0.15% C). (b) Sparks from 1045 steel (0.45% C). (c) Sparks from 1095 steel (1.0% C) More
Image
Published: 01 February 2005
Fig. 6.2 Comparison of predicted temperature in axisymmetric compression with experimental data (refer to Fig. 6.1 for locations of grid points P i,j ) (material, AISI type 1015 steel; specimen dimensions, 20 mm diam by 30 mm high; initial temperatures, 293 K). [ Lahoti et al., 1975 ] More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130563
EISBN: 978-1-62708-284-6
... 60 S 7 9260H 61 SC 7 9260 61 SC 7 9260H 90 MV 8 O2 100 C 6 E52100 CC 20 1020 CC 35 1035 CC 55 1060 XC 10 1010 XC 15 1015 XC 15 1017 XC 18 1015 XC 18 1017 XC 18 S 1023 XC 25 1023 XC 32 1034 XC 35 1034 XC 38 1034 XC 38 TS 1038...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730161
EISBN: 978-1-62708-283-9
... 2.8 18 11.7 9 13 9 5 9 7 27 72 27 81 120 180 63 50 100 90 100 Electrical resistivity, ohm m 29 ¥ 10 9 62 100 17 1011 1015 45 10 9 18 169 >1012 1012 10 5 1012 1012 50 1011 1010 1011 1012 1012 1016 1013 1016 1016 1014 1014 1012 Young s modulus, GPa 70 110 110 20 16 1050 45 113 75 205 50 14...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130537
EISBN: 978-1-62708-284-6
... 760–790 1400–1450 1012 760–790 1400–1450 1015 760–790 1400–1450 1016 760–790 1400–1450 1017 760–790 1400–1450 1018 760–790 1400–1450 1019 760–790 1400–1450 1020 760–790 1400–1450 1022 760–790 1400–1450 1513 760–790 1400–1450 1518 760–790 1400–1450...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120033
EISBN: 978-1-62708-269-3
...–995 1650–1925 Ti-6Al-2Nb-1Ta-0.8Mo 1015 1860 C 940–1050 1725–1825 B 1040–1120 1900–2050 Ti-6Al-2Sn-4Zr-2Mo(+0.2Si) (d) 990 1815 C 900–975 1650–1790 B 1010–1065 1850–1950 Ti-8Al-1Mo-1V 1040 1900 C 900–1020 1650–1870 IMI 685 (Ti-6Al-5Zr-0.5Mo-0.25Si) (e) 1030...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900031
EISBN: 978-1-62708-350-8
... for stainless steels, particularly when surface chemistry reactions are controlled (as in the plasma nitriding process), can reach 1500 HV (78 HRC). Fig. 5 The metallographic appearance of AISI 1015 (UNS G10150) steel after a 2 h vacuum nitrocarburizing treatment in an ammonia/methane mixture with 1...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130541
EISBN: 978-1-62708-284-6
... (d) … … … 1015 Rolled 11.9 (b) 12.5 (b) 13.0 (b) 13.6 (b) 14.2 (b) … … 1015 Annealed 12.2 (b) … … 13.4 (b) … 14.2 (b) … 1016 Annealed 12.0 (b) … … 13.5 (b) … 14.4 (b) … 1017 Unknown 12.2 (b) … … 13.5 (b) … 14.5 (b) … 1018 Annealed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140069
EISBN: 978-1-62708-335-5
... 96 30 99 17 57 35 0.057 0.230 963 0.33 T6 0.098 2.70 2.70 11.9 21.4 1025–1105 555–595 … 0.230 963 0.33 355.0 F 0.098 2.71 2.71 12.4 22.3 1015–1150 550–620 … … … … … … … … 0.230 963 0.33 T51 0.098 2.71 2.71 12.4 22.3 1015–1150 550–620 1155...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040025
EISBN: 978-1-62708-300-3
... 0.31 0.010 0.022 0.23 0.004 A 68 20 (c) 0.1-0.7 103.8 0.22 1015 0.15 0.40 0.01 0.016 Tr F,A 32 0 30 0.2-0.7 91.4 0.116 1015 0.15 0.40 0.01 0.016 Tr F,A 390 200 30 0.2-0.6 73.7 0.140 1015 (d) 0.15 0.40 0.045 0.045 0.25 A 68...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.9781627082846
EISBN: 978-1-62708-284-6
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120055
EISBN: 978-1-62708-269-3
... 1645 Ti-6Al-2Sn-4Zr-2Mo 995 1820 Ti-6Al-5Zr-0.5Mo-0.2Si (IMI 685) 1020 1870 Ti-5.5Al-3.5Sn-3Zr-1Nb-0.3Mo-0.3Si (IMI 829) 1015 1860 Ti-5.8Al-4Sn-3.5Zr-0.7Nb-0.5Mo-0.3Si (IMI 834) 1045 1915 Ti-6Al-2Cb-1Ta-0.8Mo 1015 1860 Ti-0.3Mo-0.8Ni (Ti code 12) 880 1615 α-β alloys...