Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-11 of 11
pH
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.t65940087
EISBN: 978-1-62708-302-7
Abstract
This chapter lays the groundwork for understanding electrode kinetics associated with corrosion. It presents a simple but useful theory relating kinetics to the polarization behavior of half-cell reactions. The theory is based on the observation that electrode potentials vary as a function of current density or charge transfer in a given area. The chapter explains how to measure and plot electrode potentials and currents and how to interpret the resulting polarization curves. It also discusses the effects of concentration gradients, explaining how they cause diffusion and, in some cases, produce changes in electrode potential.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.t65940127
EISBN: 978-1-62708-302-7
Abstract
This chapter develops a corrosion model that accounts for solution potentials and the effects of coupling between cathodic and anodic reactions. It begins by examining potential differences at various points (in the solution) along a path from the anode to the cathode area. It then presents a simple model of a galvanically coupled electrode, in which the metal is represented as an array of anode and cathode reaction surfaces. The chapter goes on to develop the related theory of mixed electrodes, showing how it can be used to predict corrosion rates based on measured potentials and current densities, polarization characteristics, and physical variables such as anode-to-cathode area ratios and fluid velocity. It also discusses the effect of corrosion inhibitors, galvanic coupling, and external currents, making extensive use of polarization curves.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.t65940233
EISBN: 978-1-62708-302-7
Abstract
This chapter discusses the principles and procedures of electrochemical measurements used to investigate corrosion behaviors. It begins by presenting a diagram of a basic potentiostatic circuit, which consists of a working electrode and an auxiliary or counter electrode suspended in an electrolytic solution. It describes how corrosion potentials and current densities are measured and explains how to deal with various sources of error. It also explains how electrochemical impedance measurements are used and describes the underlying theory and procedures in some detail.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.t65940001
EISBN: 978-1-62708-302-7
Abstract
This chapter familiarizes readers with the basic concepts of corrosion, discussing chemical reactions, ion transfer mechanisms, electrochemical processes and variables, and the formation of solid corrosion products. It presents a simple but effective teaching tool, the elementary electrochemical corrosion circuit, using it to explain how electric potential differences drive the corrosion process and how corrosion rates vary in proportion to current density. The chapter concludes with a discussion on the importance of corrosion products, such as oxides and hydroxides, and how their formation can be a major factor in controlling corrosion.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.t65940023
EISBN: 978-1-62708-302-7
Abstract
This chapter provides a thorough introduction to the electrochemical thermodynamics that govern electrode reactions associated with corrosion. It begins with a review of the thermodynamic criteria for the stability of chemical reactions based on Gibbs free energy and explains how energies of formation are determined using the oxidation of iron as an example. It then considers how iron reacts with hydrochloric acid, explaining how it can be expressed as two half reactions modeled as electrodes in an electrochemical cell. It goes on to describe the chemical reactions occurring at each electrode, accounting for different variables, mechanisms, and electrochemical effects. The chapter concludes with an in-depth review of Pourbaix diagrams, explaining what they reveal about the stability of metal-water systems and the formation of corrosion products.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.t65940183
EISBN: 978-1-62708-302-7
Abstract
This chapter discusses the complex polarization characteristics of active-passive metals and addresses related problems in interpreting their corrosion behavior. It begins by presenting several experimentally derived polarization curves for iron, comparing and contrasting them with the iron-water Pourbaix diagram. It then explains how anodic polarization is extremely sensitive to the environment and, as a result, a reasonably complete curve for a given metal-environment system usually can only be inferred. It goes on to describe how such curves are constructed, demonstrating the procedures for a wide range of alloys and environments. The examples also show how factors such as alloy concentration, crystal lattice orientation, temperature, and dissolved oxygen affect corrosion behavior.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.t65940271
EISBN: 978-1-62708-302-7
Abstract
This chapter is a detailed study of the localized corrosion behavior of steel, copper, and aluminum alloys. It applies the basic principles of electrochemistry, as well as materials science and solid and fluid mechanics, to explain the causes and effects of pitting, crevice corrosion, stress corrosion cracking, and corrosion fatigue. It describes the underlying mechanisms associated with each process and how they relate to the microstructure of the metal or alloy, the physical condition of the surface, and other factors such as the coupling of the metal to a dissimilar metal or surface film.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.t65940451
EISBN: 978-1-62708-302-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.9781627083027
EISBN: 978-1-62708-302-7
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910021
EISBN: 978-1-62708-250-1
Abstract
This chapter addresses the basic concepts important to understanding corrosion of metals. It begins with an overview of the three types of behaviors that a metal exhibits when immersed in an environment and of the four requirements of a corrosion cell. The chapter then covers the important characteristics of metals with respect to corrosion, namely the metallurgical characteristics, the inherent tendency to corrode, and the tendency to form insoluble corrosion products. The important characteristics of aqueous solutions with respect to corrosion are then addressed. The characteristics include: conductivity of the solution, acidity and alkalinity, oxidizing power, degree of ionization, and solubility in the solution. These characteristics, in combination with the characteristics of the metal, will determine the corrosion behavior of a metal/environment combination. The chapter concludes with a section on the determination of corrosion rates and corrosion rate allowances.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910193
EISBN: 978-1-62708-250-1
Abstract
Corrosive environments can be broadly classified as atmospheric, underground/soil, water, acidic, alkaline, and combinations of these. Complicating matters is the fact that there are important variables, for example, pH, temperature, and the presence of biological organisms, that can significantly alter the response of the material in a given environment. This chapter provides a detailed account of all these types of corrosion affecting various industries, pointing out the connection between the characteristics of the corrosive environment that control corrosion behavior, the corrosion characteristics of various metals and materials systems, and the subsequent corrosion response.