Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 59
Brazing
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480265
EISBN: 978-1-62708-318-8
Abstract
This chapter discusses the various methods used to join titanium alloy assemblies, focusing on welding processes and procedures. It explains how welding alters the structure and properties of titanium and how it is influenced by composition, surface qualities, and other factors. It describes several welding processes, including arc welding, resistance welding, and friction stir welding, and addresses related issues such as welding defects, quality control, and stress relieving. The chapter also covers mechanical fastening techniques along with adhesive bonding and brazing.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550511
EISBN: 978-1-62708-307-2
Abstract
Ceramics normally have high melting temperatures, excellent chemical stability and, due to the absence of conduction electrons, tend to be good electrical and thermal insulators. They are also inherently hard and brittle, and when loaded in tension, have almost no tolerance for flaws. This chapter describes the applications, properties, and behaviors of some of the more widely used structural ceramics, including alumina, aluminum titanate, silicon carbide, silicon nitride, zirconia, zirconia-toughened alumina (ZTA), magnesia-partially stabilized zirconia (Mg-PSZ), and yttria-tetragonal zirconia polycrystalline (Y-TZP). It also provides information on materials selection, design optimization, and joining methods, and covers every step of the ceramic production process.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290001
EISBN: 978-1-62708-306-5
Abstract
Joining comprises a large number of processes used to assemble individual parts into a larger, more complex component or assembly. The selection of an appropriate design to join parts is based on several considerations related to both the product and the joining process. Many product design departments now improve the ease with which products are assembled by using design for assembly (DFA) techniques, which seek to ensure ease of assembly by developing designs that are easy to assemble. This chapter discusses the general guidelines for DFA and concurrent engineering rules before examining the various joining processes, namely fusion welding, solid-state welding, brazing, soldering, mechanical fastening, and adhesive bonding. In addition, it provides information on several design considerations related to the joining process and selection of the appropriate process for joining.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290023
EISBN: 978-1-62708-306-5
Abstract
Arc welding applies to a large and diversified group of welding processes that use an electric arc as the source of heat to melt and join metals. This chapter provides a detailed overview of specific arc welding methods: shielded metal arc welding, flux cored arc welding, submerged arc welding, gas metal arc welding, gas tungsten arc welding, plasma arc welding, plasma-GMAW welding, electroslag welding, and electrogas welding. The basic characteristics of gases used for shielding during arc welding are briefly discussed.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290061
EISBN: 978-1-62708-306-5
Abstract
Resistance welding is a group of processes in which the heat for welding is generated by the resistance to the flow of an electrical current through the parts being joined. This chapter discusses the processes, advantages, and limitations of specific resistance welding processes, namely resistance spot welding, resistance seam welding, projection welding, flash welding, and upset welding.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290079
EISBN: 978-1-62708-306-5
Abstract
This chapter discusses the fusion welding processes, namely oxyfuel gas welding, oxyacetylene braze welding, stud welding (stud arc welding and capacitor discharge stud welding), high-frequency welding, electron beam welding, laser beam welding, hybrid laser arc welding, and thermit welding.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290099
EISBN: 978-1-62708-306-5
Abstract
During fusion welding, the thermal cycles produced by the moving heat source causes physical state changes, metallurgical phase transformations, and transient thermal stresses and metal movement. This chapter begins by discussing weld metal solidification behavior and the solid-state transformations of the main classes of metals and alloys during fusion welding. The main classes include work- or strain-hardened metals and alloys, precipitation-hardened alloys, transformation-hardened steels and cast irons, stainless steels, and solid-solution and dispersion-hardened alloys. The following section provides information on the residual stresses and distortion that remain after welding. The focus then shifts to distortion control of weldments. Inclusions and cracking are discussed in detail. The chapter also discusses the causes for reduced fatigue strength of a component by a weld: stress concentration due to weld shape and joint geometry; stress concentration due to weld imperfections; and residual welding stresses. Inspection and characterization of welds are described in the final section of this chapter.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290137
EISBN: 978-1-62708-306-5
Abstract
Solid-state welding processes are those that produce coalescence of the faying surfaces at temperatures below the melting point of the base metals being joined without the addition of brazing or solder filler metal. This chapter discusses solid-state welding processes such as diffusion welding, forge welding, roll welding, coextrusion welding, cold welding, friction welding, friction stir welding, explosion welding, and ultrasonic welding.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290165
EISBN: 978-1-62708-306-5
Abstract
Brazing and soldering processes use a molten filler metal to wet the mating surfaces of a joint, with or without the aid of a fluxing agent, leading to the formation of a metallurgical bond between the filler and the respective components. This chapter discusses the characteristics, advantages, and disadvantages of brazing and soldering. The first part focuses on the fundamentals of the brazing process and provides information on filler metals and specific brazing methods. The soldering portion of the chapters provides information on solder alloys used, selection criteria for base metal, the processes involved in precleaning and surface preparation, types of fluxes used, solder joint design, and solder heating methods.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290207
EISBN: 978-1-62708-306-5
Abstract
This chapter presents a comprehensive coverage of mechanical fastening methods. It begins with a discussion on the advantages and disadvantages of mechanical fastening followed by sections providing information on mechanically fastened joints and the selection of the correct fastener system. The chapter then describes important structural fasteners, namely bolts, screws, pins, collar fasteners, rivets, blind fasteners, machine pins, and spring clip fasteners. The following sections describe the process involved in presses, shrink fits, hole generation, and fastener installation. The chapter ends with information on miscellaneous mechanical fastening methods.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290243
EISBN: 978-1-62708-306-5
Abstract
Adhesive bonding is a widely used industrial joining process in which a polymeric material is used to join two separate pieces (the adherends or substrates). This chapter begins with a discussion on the advantages and disadvantages of adhesive bonding, followed by a section providing information on the theory of adhesion. The chapter then describes the considerations for designing adhesively bonded joints and for testing or characterizing adhesive materials. The following section covers the characteristics of the most important synthetic adhesive systems and five groups of adhesives, namely structural, hot melt, pressure sensitive, water based, and ultraviolet and electron beam cured. The chapter ends with a discussion on some general guidelines for adhesive bonding and the basic steps in the adhesive bonding process.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290279
EISBN: 978-1-62708-306-5
Abstract
This chapter reviews materials issues encountered in joining, including challenges involved in welding of dissimilar metal combinations; joining of plastics by mechanical fastening, solvent and adhesive bonding, and welding; joining of thermoset and thermoplastic composite materials by mechanical fastening, adhesive bonding, and, for thermoplastic composites, welding; the making of glass-to-metal seals; and joining of oxide and nonoxide ceramics to themselves and to metals by solid-state processes and by brazing. The classification, types, applications, and the mechanism of each of these methods are covered. The factors influencing joint integrity and the main considerations in welding dissimilar metal combinations are also discussed.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.9781627083065
EISBN: 978-1-62708-306-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230401
EISBN: 978-1-62708-298-3
Abstract
Beryllium has been successfully joined by fusion welding, brazing, solid-state bonding, and soldering. This chapter describes these processes in detail along with their advantages and disadvantages. It also addresses application considerations such as surface preparation, joint design, and testing.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000001
EISBN: 978-1-62708-312-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000023
EISBN: 978-1-62708-312-6
Abstract
Stainless steel powders are usually made by water or gas atomization. This chapter describes both processes and the properties and characteristics of the powders they produce. It also discusses secondary processes, including drying, screening, annealing, and lubricating, and the effects of iron contamination on corrosion resistance.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000039
EISBN: 978-1-62708-312-6
Abstract
This chapter discusses the methods by which stainless steel powders are shaped and compacted prior to sintering, including rigid die compaction, metal injection molding, extrusion, and hot isostatic pressing. It explains where each process is used and how processing parameters, such as temperature and pressure, and powder characteristics, such as particle size and shape, influence the quality of manufactured parts. It describes the various stages of metal powder compaction, the role of lubricants, and how to account for dimensional changes in the design of tooling and process sequences.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000059
EISBN: 978-1-62708-312-6
Abstract
This chapter discusses the sintering process for stainless steel powders and its influence on corrosion resistance. It begins with a review of sintering furnaces and atmospheres and the effect of temperature and density on compact properties such as conductivity, ductility, and strength. It then describes the relationship between sintered density and corrosion resistance and how it varies for different types of powders and operating environments. The chapter also explains how stainless steel powders respond to different sintering atmospheres, including hydrogen, hydrogen-nitrogen, and vacuum, and liquid-phase sintering processes.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000101
EISBN: 978-1-62708-312-6
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000109
EISBN: 978-1-62708-312-6
Abstract
This chapter discusses the mechanical properties of powder metal stainless steels and the extent to which they can be controlled through appropriate alloying and processing steps. It describes how process-related factors, such as porosity, interstitial content, sintering atmosphere, and heating and cooling profiles, affect strength, ductility, and corrosion resistance. It also provides an extensive amount of property data – including tensile and yield strength, elongation, hardness, and creep and stress rupture measurements as well as fatigue curves – for various grades of powder metal stainless steel.