Chapter 13: Heat Treating of Nonferrous Alloys
-
Published:2006
Page range:
231 - 241
Abstract
This chapter presents an overview of heat treating of nonferrous alloys. First, a brief discussion on the effects of cold work and annealing on nonferrous alloys is presented. This is followed by a discussion on the mechanisms involved in the more commonly used heat treating procedures for hardening or strengthening, namely solution treating and aging. Examples are presented for heat treating of two commercially important nonferrous alloys, one from the aluminum-copper system and one from the copper-beryllium system.
You do not currently have access to this chapter.
Citation
Heat Treating of Nonferrous Alloys, Practical Heat Treating, 2nd ed., By Jon L. Dossett, Howard E. Boyer, ASM International, 2006, p 231–241, https://doi.org/10.31399/asm.tb.pht2.t51440231
Download citation file:
Related Book Content
Metallurgy of Titanium Alloy Heat Treatment
Heat Treating of Nonferrous Alloys
Nonferrous Metals
Elementary Materials Science
Heat Treating
Titanium: A Technical Guide (Second Edition)
Problems Associated with Heat Treated Parts
Analysis and Prevention of Component and Equipment Failures
Mechanical Work of Steels—Cold Working
Metallography of Steels Interpretation of Structure and the Effects of Processing
Thermal Processing
Stainless Steels for Design Engineers
General Introduction to Casting
Metals Handbook Desk Edition (2nd Edition)
Approximate Composition of Materials
Extrusion (Second Edition)
Corrosion Resistance of Aluminum Alloys
Corrosion in the Petrochemical Industry (Second Edition)
Stress-Corrosion Cracking of Copper Alloys
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)