Book Chapter
Chapter 10: Heat Treating of Stainless Steels
-
Published:2006
Page range:
175 - 190
Abstract
This chapter discusses the processes involved in heat treating of stainless steels, providing information on the classification, chemical compositions, and corrosion resistance of stainless steels and the effect of specific elements on the characteristics of iron-base alloys. Five groups of stainless steels are discussed: austenitic, ferritic, martensitic, precipitation-hardening, and duplex grades. The chapter also describes the heat treatment conditions that should be maintained for processing of stainless steels.
You do not currently have access to this chapter.
Citation
Heat Treating of Stainless Steels, Practical Heat Treating, 2nd ed., By Jon L. Dossett, Howard E. Boyer, ASM International, 2006, p 175–190, https://doi.org/10.31399/asm.tb.pht2.t51440175
Download citation file:
Related Book Content
Stainless Steels
Steel Metallurgy for the Non-Metallurgist
Corrosion in the Food and Beverage Industries
Corrosion: Environments and Industries
Corrosion Resistance of Stainless Steels and Nickel Alloys
Corrosion: Fundamentals, Testing, and Protection
Corrosion of Stainless Steel Weldments
Corrosion in the Petrochemical Industry (Second Edition)
Stainless Steels
Steels: Processing, Structure, and Performance (Second Edition)
Corrosion Theory
Stainless Steels for Design Engineers
Crevice Corrosion
Corrosion in the Petrochemical Industry (Second Edition)
Architecture and Construction
Stainless Steels for Design Engineers
Corrosion Resistance of Magnesium Alloys
Corrosion in the Petrochemical Industry (Second Edition)
Temperature Requirements for Heating Super Alloys and Stainless Steels
Induction Heating and Heat Treatment