Abstract
The relationship of stress and strength gradients must be considered simultaneously in analysis of a particular type of fracture. This chapter discusses the principal elastic stress distribution in members of various shapes under different types of pure loads. A basic understanding of both the stress and strength gradients of metal parts with and without stress concentrations and under different types of loading is provided. The chapter also describes the effect of service conditions on applied stresses.
Topics
Deformation and fracture
You do not currently have access to this chapter.
Citation
Stress versus Strength, Understanding How Components Fail, 3rd ed., By Donald J. Wulpi;Edited By Brett Miller, ASM International, 2013, p 23–33, https://doi.org/10.31399/asm.tb.uhcf3.t53630023
Download citation file:
Related Book Content
Evaluation of Workability for Bulk Forming Processes
Metalworking: Bulk Forming
Techniques of Failure Analysis
Understanding How Components Fail (Third Edition)
Age Forming
Metalworking: Sheet Forming
Failure Analysis of Open End Wrenches Containing Forging Defects
Handbook of Case Histories in Failure Analysis
Effects of Metallurgical Variables on Aqueous Corrosion
Corrosion: Fundamentals, Testing, and Protection
Fatigue Fracture
Understanding How Components Fail (Third Edition)
Flanging of Aluminum
Metalworking: Sheet Forming
Deformation, Mechanical Properties, and Fracture of Quenched and Tempered Carbon Steels
Steels: Processing, Structure, and Performance (Second Edition)
Fracture and Fractography of Elastomeric Materials
Characterization and Failure Analysis of Plastics
Stress Systems Related to Single-Load Fracture of Ductile and Brittle Metals
Understanding How Components Fail (Third Edition)