Abstract
Failure analysis is a systematic investigative procedure using the scientific method to identify the causes of a failure. This chapter begins by exploring what failure analysis is followed by a section describing the sequence of stages in the investigation and analysis of failure and the three principles that must be carefully followed during the analysis. It then provides information on the normal location of fracture and concludes with a list of questions to ask about fractures.
You do not currently have access to this chapter.
Citation
Techniques of Failure Analysis, Understanding How Components Fail, 3rd ed., By Donald J. Wulpi;Edited By Brett Miller, ASM International, 2013, p 1–12, https://doi.org/10.31399/asm.tb.uhcf3.t53630001
Download citation file:
Related Book Content
General Aspects of Failure Analysis
Failure Analysis of Heat Treated Steel Components
Failure Analysis of Open End Wrenches Containing Forging Defects
Handbook of Case Histories in Failure Analysis
Failure Analysis of Medical Devices
Analysis and Prevention of Component and Equipment Failures
Flanging of Aluminum
Metalworking: Sheet Forming
Fracture and Fractography of Elastomeric Materials
Characterization and Failure Analysis of Plastics
Stress versus Strength
Understanding How Components Fail (Third Edition)
Deformation, Mechanical Properties, and Fracture of Quenched and Tempered Carbon Steels
Steels: Processing, Structure, and Performance (Second Edition)
Crazing and Fracture in Polymers
Characterization and Failure Analysis of Plastics
Failure of Rockbolts in Underground Mines in Australia
ASM Failure Analysis Case Histories: Construction, Mining, and Agricultural Equipment
Residual Strength of Metal Structures
Fatigue and Fracture