Abstract
Designs and materials continue to become more complex, with novel technologies developed to create them, and novel instruments invented to analyze them. Engineers at all stages of the design and manufacturing process should appreciate the reasons why formal failure analysis is performed. This chapter describes why failure analysis is conducted and outlines the responsibilities of the failure analyst.
You do not currently have access to this chapter.
Citation
Why Perform Failure Analysis?, Understanding How Components Fail, 3rd ed., By Donald J. Wulpi;Edited By Brett Miller, ASM International, 2013, p xvi–xix, https://doi.org/10.31399/asm.tb.uhcf3.t53630xvi
Download citation file:
Related Book Content
Engineering Design Process Investigation in a Failure Analysis
Analysis and Prevention of Component and Equipment Failures
Failure Causes
Composites
Training Needs for the Failure Analyst
Microelectronics Failure Analysis: Desk Reference (Seventh Edition)
Manufacturing Cost Estimating
Metals Process Simulation
Metal Forming Processes in Manufacturing
Cold and Hot Forging Fundamentals and Applications
Design for Deformation Processing
Metalworking: Bulk Forming
Engineering for Functional Performance
Iron and Steel Castings Engineering Guide
Design and Manufacturing Implications of Additive Manufacturing
Additive Manufacturing Processes
Process and Feedback Control for Manufacturing
Metalworking: Sheet Forming
Solid Modeling
Metals Process Simulation