Book Chapter
Chapter 3: Systems and Systems Failure Analysis Concepts
-
Published:2009
Abstract
A system failure occurs when a system does not do what it is supposed to do when it is supposed to do it, or it does something it is not supposed to do. This chapter provides a basic understanding of how failures occur, how systems operate, and the types of failures, namely intermittent and inadvertent system failures.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Systems and Systems Failure Analysis Concepts, Systems Failure Analysis, By Joseph Berk, ASM International, 2009, p 19–24, https://doi.org/10.31399/asm.tb.sfa.t52780019
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Failure Analysis Terms and Definitions
Microelectronics Failure Analysis: Desk Reference (Seventh Edition)
The Failure Analysis Process: An Overview
Failure Analysis and Prevention
Failure Analysis: Why and for Whom?
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure Analysis and After
Failure Analysis of Engineering Structures Methodology and Case Histories
Glossary of Terms—Failure Analysis and Prevention
Failure Analysis and Prevention (2021 Edition)
Component Failure Causes and Suggested Analysis Methods
Systems Failure Analysis
Techniques of Failure Analysis
Understanding How Components Fail (Third Edition)
Failure Analysis Methodology
Failure Analysis of Engineering Structures Methodology and Case Histories
The Failure Analysis Process—An Overview
Failure Analysis and Prevention (2021 Edition)
Abrasive Wear Failures
Failure Analysis and Prevention (2021 Edition)