Steel Metallurgy for the Non-MetallurgistAvailable to Purchase
ASM International
ISBN electronic:
978-1-62708-264-8
Publication date:
2007
Book Chapter
Chapter 5: Mechanical Properties Available to Purchase
-
Published:2007
Page range:
39 - 54
Abstract
Metals are used in many engineering applications because of their mechanical properties, particularly strength and ductility. This chapter explains how mechanical properties are measured and how to interpret the results. It describes the most widely used tests, including tensile tests; Rockwell, Brinell, Vickers, and Knoop hardness tests; and Charpy V-notch impact tests. The chapter also provides information on loading conditions that can lead to fatigue failure, and in some cases, counteract or prevent it.
You do not currently have access to this chapter.
Citation
Mechanical Properties, Steel Metallurgy for the Non-Metallurgist, By John D. Verhoeven, ASM International, 2007, p 39–54, https://doi.org/10.31399/asm.tb.smnm.t52140039
Download citation file:
Related Book Content
Tensile Testing
Inspection of Metals Understanding the Basics
Comparison of Hardness Tests
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Tensile Testing of Metals and Alloys
Tensile Testing (Second Edition)
Structure-Properties Relationships in Metal Additive Manufacturing
Additive Manufacturing Design and Applications
Steel Heat Treatment Failures due to Quenching
Quenchants and Quenching Technology
Introduction to Carburizing and Carbonitriding
Steel Heat Treating Fundamentals and Processes
Stress-Relief Heat Treating of Steel
Steel Heat Treating Fundamentals and Processes
Residual Stresses in Induction Hardened Steels
Induction Heating and Heat Treatment
Residual Stress
Quenchants and Quenching Technology
Mechanical Testing and Properties of Plastics: An Introduction
Characterization and Failure Analysis of Plastics