Chapter 1: Introduction to Boiler Technology
-
Published:2018
Abstract
Boilers are engineered systems designed to convert the chemical energy in fuel into heat to generate hot water or steam. This chapter describes boiler applications and types, including firetube boilers, watertube boilers, electric boilers, packaged boilers, fluidized bed combustion boilers, oil- and gas-fired boilers, waste heat boilers, and black liquor recovery boilers. It also describes the operation and working principle of utility or power plant boilers, covering conventional subcritical and advanced supercritical types.
Introduction to Boiler Technology, Failure Investigation of Boiler Tubes: A Comprehensive Approach, By Paresh Haribhakti, P.B. Joshi, Rajendra Kumar, ASM International, 2018, p 1–16, https://doi.org/10.31399/asm.tb.fibtca.t52430001