Titanium alloys are classified according to the amount of alpha and beta phase material retained in their structures at room temperature. This chapter discusses the metallurgy, composition, processing, and properties of titanium and its alloys. It provides information on melting, forging, casting, heat treating, and secondary fabrication. It also discusses the advantages and disadvantages of titanium and its alloys in various applications.
You do not currently have access to this chapter.
Citation
Titanium, Elements of Metallurgy and Engineering Alloys, Edited By F.C. Campbell, ASM International, 2008, p 527–545, https://doi.org/10.31399/asm.tb.emea.t52240527
Download citation file:
Related Book Content
Aluminum
Elements of Metallurgy and Engineering Alloys
Superalloys
Elements of Metallurgy and Engineering Alloys
Foundry Practice for Nonferrous Alloys
Metals Handbook Desk Edition (2nd Edition)
Listing of Selected Specification and Standardization Organizations
Titanium: A Technical Guide (Second Edition)
Processing of Titanium and Titanium Alloys
Metals Handbook Desk Edition (2nd Edition)
Forging and Forming
Titanium: A Technical Guide (Second Edition)
Titanium and Its Alloys for Biomedical Implants
Materials for Medical Devices
Casting, Forming, and Forging
Gear Materials, Properties, and Manufacture
Corrosion Data
Titanium: A Technical Guide (Second Edition)
Machining Data
Titanium: A Technical Guide (Second Edition)