This chapter discusses the process characteristics, advantages, disadvantages, and applications of various processes involved in surface hardening of steel. These include pack carburizing, liquid carburizing, gas carburizing, vacuum carburizing, plasma carburizing, gas nitriding, liquid nitriding, carbonitriding, and hardfacing. The chapter describes two surface hardening processes by localized heat treatment: flame hardening and induction hardening. It also briefly summarizes other surface hardening processes, namely, aluminizing, siliconizing, chromizing, titanium carbide coatings, and boronizing.