Precipitation hardening is used extensively to strengthen aluminum alloys, magnesium alloys, nickel-base superalloys, beryllium-copper alloys, and precipitation-hardening stainless steels. This chapter discusses two types of particle strengthening: precipitation hardening, which takes place during heat treatment; and true dispersion hardening, which can be achieved by mechanical alloying and powder metallurgy consolidation. It provides information on the three steps of precipitation hardening of aluminum alloys: solution heat treating, rapid quenching, and aging.