Abstract
When a metal is alloyed with another metal, either substitutional or interstitial solid solutions are usually formed. This chapter discusses the general characteristics of these solutions and the effects of several alloying elements on the yield strength of pure metals. It presents four rules that give a qualitative estimate of the ability of two metals to form substitutional solid solutions: relative size factor, chemical affinity factor, relative valency factor, and lattice type factor. The chapter provides information on alloys that form an ordered structure during heating. It describes the intermediate phases that are formed during solidification between the two...
Sign in
ASM members
Member Sign InSolid Solutions, Elements of Metallurgy and Engineering Alloys, Edited By F.C. Campbell, ASM International, 2008, p 41–52, https://doi.org/10.31399/asm.tb.emea.t52240041
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.