Elements of Metallurgy and Engineering Alloys
Chapter 1: Metallic Structure
-
Published:2008
Abstract
Bonding in solids may be classified as either primary or secondary bonding. Methods of primary bonding include the metallic, ionic, and covalent bonds. This chapter discusses and provides a comparison of the properties of these bonds. This is followed by a discussion on crystalline structure, providing information on space lattices and crystal systems, hexagonal close-packed systems, and face-centered and body-centered cubic systems. The chapter then covers slip systems and closes with a brief section on allotropic transformations that occur at a constant temperature during either heating or cooling.
Sign in
ASM members
Member Sign InMetallic Structure, Elements of Metallurgy and Engineering Alloys, Edited By F.C. Campbell, ASM International, 2008, p 3–16, https://doi.org/10.31399/asm.tb.emea.t52240003
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.