Elements of Metallurgy and Engineering AlloysAvailable to Purchase
Elements of Metallurgy and Engineering Alloys provides thorough and systematic coverage of basic metallurgy and the practical engineering aspects of metallic material selection and application. The coverage of the book includes practical information on the engineering properties and applications of steels, cast irons, nonferrous alloys, and metal matrix composites; concise overviews and practical implications of metallic structure, imperfections, deformation, and phase transformations; process metallurgy of solidification and casting, recovery, recrystallization and grain growth, and precipitation hardening; mechanical deformation during processing; in-service properties of fatigue, fracture, and creep; and physical properties and corrosion. For information on the print version, ISBN 978-0-87170-867-0, follow this link.
Download citation file:
Table of Contents
-
Part I: Physical and Mechanical Metallurgy
-
Part II: Engineering Alloys
-
Part III: Reference Information