Microelectronics Failure Analysis: Desk Reference (Seventh Edition)
Package Failure Analysis: Flow and Technique
-
Published:2019
Abstract
As semiconductor feature sizes have shrunk, the technology needed to encapsulate modern integrated circuits has expanded. Due to the various industry changes, package failure analyses are becoming much more challenging; a systematic approach is therefore critical. This article proposes a package failure analysis flow for analyzing open and short failures. The flow begins with a review of data on how the device failed and how it was processed. Next, non-destructive techniques are performed to document the condition of the as-received units. The techniques discussed are external optical inspection, X-ray inspection, scanning acoustic microscopy, infrared (IR) microscopy, and electrical verification....
Sign in
ASM members
Member Sign InTejinder Gandhi, Jason Silva, Package Failure Analysis: Flow and Technique, Microelectronics Failure Analysis: Desk Reference, 7th ed., Edited By Tejinder Gandhi, ASM International, 2019, p 10–15, https://doi.org/10.31399/asm.tb.mfadr7.t91110010
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!