This chapter discusses how aluminum and other alloying constituents are added to prepare a furnace charge for the melting process, and how it is cast into billets of various aluminum alloys. Fundamental aspects of billet casting are covered to give an overview of the casting process. The melting practice is discussed, as well as grain refining and degassing. Charge material, grain refining, degassing, filtration of melt, casting systems, and casting variables are discussed. The chapter concludes with a discussion of casting defects.