This chapter explores case studies on using induction heating for joining applications, encompassing both soldering and brazing to demonstrate versatility. Each study focuses on inductor coil design, workpiece geometry, and production quantities, emphasizing optimization due to the interplay between material geometry, coil configuration, and process parameters like generator frequency and power. The case studies provide real-world data on effectively implementing induction heating in joining processes.