Chapter 2: A Brief Review of the History of Brazing and Soldering
-
Published:2024
Abstract
This chapter presents a brief review of the history of brazing and soldering. It illustrates complicated soldering techniques and masterful goldsmith work, as demonstrated by the famous gold mask of the Egyptian Pharaoh Tutankhamun. The chapter includes the image of a painting from Egypt circa 1475 B.C. that shows a goldsmith soldering with a blowpipe. Numerous similar images have been found in the tombs of ancient Egypt that offer insight into the practices of gold workers from the period, including the use of processes such as smelting, forging, and joining with both brazing and soldering.
A Brief Review of the History of Brazing and Soldering, Handbook of Induction Soldering: Principles, Processing, and Applications, By Hans-Joachim Peter;Edited By Paul T. Vianco, ASM International, 2024, p 5–10, https://doi.org/10.31399/asm.tb.hisppa.t56110005