Abstract
Integrated computational materials engineering (ICME) is a novel approach to design, develop, and deploy materials. This chapter presents ICME and the development of third generation advanced high-strength steels.
Topics
Advanced high-strength steel
You do not currently have access to this chapter.
Citation
Integrated Computational Materials Engineering Approach to Advanced High-Strength Steels Development, Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition, By Mahmoud Y. Demeri, ASM International, 2024, p 319–323, https://doi.org/10.31399/asm.tb.ahsssta2.t59410319
Download citation file:
Related Book Content
Advanced Steels for Forming Operations
Metallography of Steels Interpretation of Structure and the Effects of Processing
Applications of Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Global Projects on Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Evolving Grades of Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Introduction to Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Design Guidelines for Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Sustainability and Economics of Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Nanosteels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Forming of Advanced High-Strength Steels (AHSS)
Sheet Metal Forming Processes and Applications